| PAN Hongge; CHEN Yun; CHEN Changpin(Department of Materials Science and Eegineering; Zhejiang University; Hangzhou 310027)YANG Fuming(State Key Laboratory for Magnetism; Institute of Physics; The Chinese Academy of Sciences; Beijing 100080)Correspondent: PAN Hongge; Tel: (0571)7951406 Fax: (0571)7951152 |
引用本文:
潘洪革;陈昀;陈长聘;杨伏明. SmFe_(10.7-x)Mo_(1.3)Ga_x化合物的结构与内禀磁性[J]. 金属学报, 1998, 34(8): 836-840.
,
,
,
.
STRUCTURAL CHARACTERIZATION AND INTRINSIC MAGNETIC PROPERLIES OF THE SmFe_(10.7-x)Mo_(1.3)Ga_x COMPOUNDS[J]. Acta Metall Sin, 1998, 34(8): 836-840.
1 Middleton D F, Mishra S R, Long G J, Pringle O A, Hu Z, Yelon W B, Grandjean F, Buschow K H J.J Appl Phys, 1995; 78: 5568 2 Rogalski M S, Morariu M, Valeanu M, Plugurn N. Solid State Commun, 1993; 87: 139 3 Li Z W, Zhou Z, Morrish A H. Phys Rev, 1995; 51B: 2891 4 Sabirianor R F, Jaswal S S. J Appl Phys, 1996; 79: 5942 5 Coehoorn R. Phys Rev, 1990; 41B: 1790 6 Mooji D B, Buschow K H J. J Less-Common Met, 1988; 131: 207 7 成昭华.中国科学物理研究所博士学位论文, 1995(Chen Z H, Ph D Thesis, Institute of Physics, The Chinese Academy of Sciences, Beijing, 1995)j |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|