Please wait a minute...
金属学报  1998, Vol. 34 Issue (8): 836-840    
  论文 本期目录 | 过刊浏览 |
SmFe_(10.7-x)Mo_(1.3)Ga_x化合物的结构与内禀磁性
潘洪革;陈昀;陈长聘;杨伏明
浙江大学材料科学与工程学系;杭州;310027;浙江大学材料科学与工程学系;杭州;310027;浙江大学材料科学与工程学系;杭州;310027;中国科学院物理研究所磁学国家重点实验室;北京;100080
STRUCTURAL CHARACTERIZATION AND INTRINSIC MAGNETIC PROPERLIES OF THE SmFe_(10.7-x)Mo_(1.3)Ga_x COMPOUNDS
PAN Hongge; CHEN Yun; CHEN Changpin(Department of Materials Science and Eegineering; Zhejiang University; Hangzhou 310027)YANG Fuming(State Key Laboratory for Magnetism; Institute of Physics; The Chinese Academy of Sciences; Beijing 100080)Correspondent: PAN Hongge; Tel: (0571)7951406 Fax: (0571)7951152
引用本文:

潘洪革;陈昀;陈长聘;杨伏明. SmFe_(10.7-x)Mo_(1.3)Ga_x化合物的结构与内禀磁性[J]. 金属学报, 1998, 34(8): 836-840.
, , , . STRUCTURAL CHARACTERIZATION AND INTRINSIC MAGNETIC PROPERLIES OF THE SmFe_(10.7-x)Mo_(1.3)Ga_x COMPOUNDS[J]. Acta Metall Sin, 1998, 34(8): 836-840.

全文: PDF(429 KB)  
摘要: 本文详细研究了Ga取代Sm(R,Mo)12化合物中的部分Fe对其结构和内禀磁性的影响.其中包括:Ga在Sm(Fe,Mo)12化合物中的原子占位,不同Ga取代对SmFe10.7-xMo1.3Gax化合物的晶胞常数,Curie温度,饱和磁化强度,磁晶各向异性的影响.实验结果表明:Ga替代增加晶胞体积,降低Curie温度,减小饱合磁化强度,降低Fe原子的平均磁矩;随Ga含量的提高,SmFe10.7-xMo1.3Gax化合物由单轴向锥面各向异性转变
关键词 Sm(Fe,Mo)_(12)化合物Ga掺杂内禀磁性    
Abstract:The structural characterization and intrinsic magnetic properties of the compounds SmFe10.7-x Mo1.3Gax have been investigated in great detail, which included the lattice parameters, Curie temperature TC, saturation magnetization σs, and magnetocrystallize anisotropy. The results indicate that Ga occupies 8j and 8f sites, and substitution of Ga for Fe in SmFe10.7Mo1.3 leads to the expansion of the lattice constants a, c and unit cell volume V, the monotonical decrease of the Curie temperature TC, and the decrease of saturation magnetization and the Fe moments. The magnetocrystalline anisotropy changes from uniaxial to conical plane.
Key wordsSm(Fe    Mo)_(12)    Ga substitution    intrinsic magnetic property
收稿日期: 1998-08-18     
1 Middleton D F, Mishra S R, Long G J, Pringle O A, Hu Z, Yelon W B, Grandjean F, Buschow K H J.J Appl Phys, 1995; 78: 5568
2 Rogalski M S, Morariu M, Valeanu M, Plugurn N. Solid State Commun, 1993; 87: 139
3 Li Z W, Zhou Z, Morrish A H. Phys Rev, 1995; 51B: 2891
4 Sabirianor R F, Jaswal S S. J Appl Phys, 1996; 79: 5942
5 Coehoorn R. Phys Rev, 1990; 41B: 1790
6 Mooji D B, Buschow K H J. J Less-Common Met, 1988; 131: 207
7 成昭华.中国科学物理研究所博士学位论文, 1995(Chen Z H, Ph D Thesis, Institute of Physics, The Chinese Academy of Sciences, Beijing, 1995)j
No related articles found!