					引用本文:
						|  |  
    					|  |  
    					| Mo粉表面化学镀Cu及其反应机理 |  
						| 王光君; 王德志; 周杰;  吴壮志; 徐兵 |  
					| 1. 中南大学有色金属材料科学与工程教育部重点实验室; 长沙 410083 2. 中南大学 材料科学与工程学院; 长沙 410083
 |  
						|  |  
    					| ELECTROLESS PLATING Cu ON Mo POWDER AND ITS REACTION MECHANISM |  
						| WANG Guangjun; WANG Dezhi; ZHOU Jie; WU Zhuangzhi; XU Bing |  
						| 1. Key Laboratory of Nonferrous Metal Materials Science and Engineering; Ministry of Education; Central South University; Changsha 410083 2. School of Materials Science and Engineering; Central South University; Changsha 410083
 |  
								王光君  王德志  周 杰  吴壮志 徐兵. Mo粉表面化学镀Cu及其反应机理[J]. 金属学报, 2009, 45(4): 405-409.	
																												,
																												 . 
				ELECTROLESS PLATING Cu ON Mo POWDER AND ITS REACTION MECHANISM[J]. Acta Metall Sin, 2009, 45(4): 405-409.
 
					
						| 
								
									|  
          
          
            
                         
            
									            
									                
																														  
																| [1] Lu D M. Powder Metall Ind, 2002; 10(6): 30(吕大铭. 粉末冶金工业, 2002; 10(6): 30)
 [2] Maneshian M H, Simchi A, Razavi H Z. Mater Sci Eng, 2007; A445–446: 86
 [3] Hwang K S, Huang H S. Mater Chem Phys, 2001; 67: 92
 [4] Gusmano G, Bianco A, Polini R, Magistris P, Marcheselli G. J Mater Sci, 2001; 30: 901
 [5] Raghu T, Sundaresan R, Ramakrishnan P, Ramamohan T R. Mater Sci Eng, 2001; A304–36: 438
 [6] Peng X L. Mater Sci Eng, 1999; A262: 1
 [7] Wang H Q, Li X H, Guo H J, Zhang B, Guo Y X. J Cent South Univ(Sci Technol), 2003; 34: 615
 (王红强, 李新海, 郭华军, 张宝, 郭永兴. 中南大学学报(自然科学版), 2003; 34: 615)
 [8] Sharma R, Agarwala R C, Agarwala V. Appl Surf Sci, 2006; 252: 8487
 [9] Lee W, Yang H J, Reucroft P J, Soh H S, Kim J H, Woo S L, Lee J. Thin Solid Films, 2001; 392: 122
 [10] Shukla S, Seal S, Akesson J, Oder R, Carter R, Rahman Z. Appl Surf Sci, 2001; 181: 35
 [11] Meenan B J, Brown N M D, Wilson J W. Appl Surf Sci, 1994; 74: 221
 [12] Huang H Z. The Surface Chemical Analysis. Shanghai: East China University of Science and Technology Press, 2001: 21
 (黄惠忠. 表面化学分析. 上海: 华东理工大学出版社, 2001: 21)
 |  
             
												
											    	
											        	|  | Viewed |  
											        	|  |  |  
												        |  | Full text 
 | 
 
 |  
												        |  |  |  
												        |  | Abstract 
 | 
 |  
												        |  |  |  
												        |  | Cited |  |  
												        |  |  |  |  
													    |  | Shared |  |  
													    |  |  |  |  
													    |  | Discussed |  |  |  |  |