| NiAl--Cr(Mo)--Ho--Hf共晶合金的高温磨损特性 |
| 王振生1;2;郭建亭1;周兰章1;盛立远1;胡壮麒1 |
1 中国科学院金属研究所; 沈阳 110016
2 湖南科技大学机电工程学院; 湘潭 411201 |
|
| HIGH TEMPERATURE WEAR BEHAVIOR OF NiAl--Cr(Mo)--Ho--Hf EUTECTIC ALLOY |
| WANG Zhensheng1;2;GUO Jianting1;ZHOU Lanzhang1;SHENG Liyuan1;HU Zhuangqi1 |
1 Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016
2 School of Electromechanical Engineering; Hunan University of Science and Technology; Xiangtan 411201 |
引用本文:
王振生 郭建亭 周兰章 盛立远 胡壮麒. NiAl--Cr(Mo)--Ho--Hf共晶合金的高温磨损特性[J]. 金属学报, 2009, 45(3): 297-301.
,
,
,
,
.
HIGH TEMPERATURE WEAR BEHAVIOR OF NiAl--Cr(Mo)--Ho--Hf EUTECTIC ALLOY[J]. Acta Metall Sin, 2009, 45(3): 297-301.
| [1] Guo J T. Ordered Intermetallic Compound NiAl Alloy. Beijing: Science Press, 2003: 75
(郭建亭. 有序金属间化合物镍铝合金. 北京: 科学出版社, 2003: 75)
[2] Johnson B J, Kennedy F E, Baker I. Wear, 1996; 192: 241
[3] Hawk J A, Alman D E. Mater Sci Eng, 1997; A239–240: 899
[4] Hawk J A, Alman D E. Wear, 1999; 225–229: 544
[5] Wang Z S, Zhou L Z, Guo J T, Sheng L Y, Hu Z Q. Tribology, 2008; 28: 497
(王振生, 周兰章, 郭建亭, 盛立远, 胡壮麒. 摩擦学学报, 2008; 28: 497)
[6] Jiang X X, Li S Z, Li S. Corrosive Wear of Metals. Beijing: Chemical Industry Press, 2003: 78
(姜晓霞, 李诗卓, 李曙. 金属的腐蚀磨损. 北京: 化学工业出版社, 2003: 78)
[7] Kingery W D, Bowen H K, Uhlmann D R, Translated by
Zhuang B Q. Ceramic Introduction. Beijing: China Architecture and Building Press, 1987: 368
(Kingery W D, Bowen H K, Uhlmann D R, 著; 庄炳群, 译. 陶瓷导论. 北京: 中国建筑工业出版社, 1987: 368)
[8] Liu R T, Li X B, Cheng S H. Chin J Nonferrous Met, 2003; 13: 469
(刘如铁, 李溪滨, 程时和. 中国有色金属学报, 2003; 13: 469)
[9] Stott F H, Glascott J, Wood G C. Wear, 1985; 101: 311
[10] Jiang J R, Stott F H, Stack M M. Wear, 1994; 176: 185
[11] Ouyang J H, Sasaki S, Murakami T, Umeda K. Ceram Int, 2005; 31: 543 |
|