| 多晶铝轧制变形的织构演变I. 实验研究 |
| 陈志永;才鸿年;常亚喆;张新明;刘楚明 |
| 中南大学材料科学与工程学院 |
|
| TEXTURE EVOLUTION OF POLYCRYSTALLINE ALUMINUM DURING ROLLING DEFORMATION - I. Experimental Study |
| Zhiyong Chen;;;; |
| 中南大学 |
引用本文:
陈志永; 才鸿年; 常亚喆; 张新明; 刘楚明 . 多晶铝轧制变形的织构演变I. 实验研究[J]. 金属学报, 2008, 44(11): 1316-1321 .
,
,
,
,
.
TEXTURE EVOLUTION OF POLYCRYSTALLINE ALUMINUM DURING ROLLING DEFORMATION - I. Experimental Study[J]. Acta Metall Sin, 2008, 44(11): 1316-1321 .
[1]Sachs E.Z Vet Deut Ing,1928;72:734 [2]Taylor G I.J Inst Met,1938;62:307 [3]Honneff H,Mecking H.In:Gottstein G,L(?)cke K,eds., Proc 5th Int Conf on Textures of Materials,Aachen: Springer,1978:265 [4]van Houtte P.In:Nagashima S,ed.,Proc 6th Int Conf on Teztures of Materials,Tokyo:Iron and Steel Institute of Japan,1981:428 [5]Kocks U F,Chandra H.Acta Metall,1982;30:695 [6]Fortunier R,Driver J H.Acta Metall,1987;35:509 [7]Kocks U F.Metall Trans,1970;1:1121 [8]Hirsch J,L(?)cke K.Acta Metall,1988;36:2883 [9]Zhang X M,Li S Y.Bull Natl Nat Sci Found China,1995; 9(3):26 (张新明,李赛毅.中国科学基金,1995;9(3):26) [10]Kalidindi S R,Bronkhorst C A,Anand L.J Mech Phys Solids,1992;40:537 [11]Engler O,Huh M Y,Tome C N.Metall Mater Trans,2000; 31A:2299 [12]Raabe D,Zhao Z,Mao W.Acta Mater,2002;50:4379 [13]Zhao Z,Kuchnicki S,Radovitzky R,Cuitino A.Acta Mater,2007;55:2361 [14]Cao P,Fan G,Lei L P,Zeng P.Acta Metall Sin,2007;43: 913 (曹鹏,方刚,雷丽萍,曾攀.金属学报,2007;43:913) [15]Bishop J F W,Hill R.Philos Mag,1951;42:414 [16]Bishop J F W,Hill R.Philos Mag,1951;42:1298 [17]Bunge H J.Leffers T.Scr Metall,1971;5:143 [18]Mecking H.In:Nagashima S,ed.,Proc 6th Int Conf on Textures of Materials,Tokyo:Iron and Steel Institute of Japan,1981:53 [19]Canova G R,Kocks U F.In:Brakman C M,Jongenburger P,Mittemeijer E J,eds.,Proc 7th Int Conf on Textures of Materials.Noordwijkerhout:Netherlands Society of Ma- terials Science,1984:573 [20]Asaro R J,Needleman A.Acta Metall,1985;33:923 [21]Renouard M,Wintenberger M.C R Acad Sci,1976;283B: 237 [22]Busso Esteban P,Cailletaud G.Int J Plast,2005;21:2212 [23]Bunge H J.Texture Analysis in Materials Science Mathematical Methods.London:Butterworths.1982:47 [24]L(?)cke K,Pospiech J,Virnich K H,Jura J.Acta Metall, 1981;29:167 [25]Hirsch J,L(?)cke K,Hatherly M.Acta Metall,1988;36: 2905 [26]Chen Z Y,Cai H N,Chang Y Z,Zhang X M,Liu C M. Acta Metall Sin,2008;44:1322 (陈志水,才鸿年,常亚喆,张新明,刘楚明.金属学报,2008;44:1322) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|