| 旋流水口对小方坯连铸结晶器流场影响的水模拟研究 |
| 贾洪海 于 湛 雷作胜 邓 康 陈家昶 华文杰 任忠鸣 |
| 上海大学材料学院 |
|
| Effect of Swirling Flow out of Nozzle on Flow Field in Continuous Casting of Billet |
引用本文:
贾洪海; 于湛; 雷作胜; 邓康; 陈家昶; 华文杰; 任忠鸣 . 旋流水口对小方坯连铸结晶器流场影响的水模拟研究[J]. 金属学报, 2008, 44(3): 375-380 .
[1]Yokoya S,Asako Y,Hara S,Szekely J.ISIJ Int,1994;34: 883 [2]Yokoya S,Westoff R,Asako Y,Hara S,Szekely J.ISIJ Int,1994;34:889 [3]Yeong H H.ISIJ Int,1996;36:1030 [4]Yokoya S,Takagi S,Iguchi M,Asako Y,Westoff R,Hara S.ISIJ Int,1998;38:827 [5]Yokoya S,Takagi S,Iguchi M,Marukawa K,Yasugaira W, Hara S.ISIJ Int,2000;40:584 [6]Yokoya S,Takagi S,Tada K,Iguchi M,Marukawa K,Hara S.ISIJ Int,2001;41:1201 [7]Yokoya S,Takagi S,Ootani S,Iguchi M,Marukawa K, Hara S.ISIJ Int,2001;41:1208 [8]Yokoya S.ISIJ Int,2001;41(Suppl.):S47 [9]Zhang H,Wang T F,Wang J F,Jin Y.J Chem Eng Chin Univ,2002;16:408 (张欢,王铁峰,王金福,金涌.高校化学工程学报,2002;16:408) [10]Yu Z,Lei Z S,Jia H H,Jin X L,Ren Z M,Deng K,Zhong Y B.Shanghai Met,2007;29(2):54 (于湛,雷作胜,贾洪海,金小礼,任忠鸣,邓康,钟云波.上海金属,2007;29(2):54) [11]Li B K,Li D H.Acta Metall Sin,2002;38:315 (李宝宽,李东辉.金属学报,2002;38:315) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|