| 调制结构对TiN/TaN多层膜的生长行为及力学性能的影响 |
| 赵阳; 王 娟; 徐晓明;张庆瑜 |
| 大连理工大学 |
|
| Influence of modulation structure on the growth behavior, structural characterization and mechanical properties of TiN/TaN multilayers |
| Qingyu Zhang |
| 大连理工大学 |
引用本文:
赵阳; 王娟; 徐晓明; 张庆瑜 . 调制结构对TiN/TaN多层膜的生长行为及力学性能的影响[J]. 金属学报, 2006, 42(4): 389-393 .
,
,
,
.
Influence of modulation structure on the growth behavior, structural characterization and mechanical properties of TiN/TaN multilayers[J]. Acta Metall Sin, 2006, 42(4): 389-393 .
[1] Yashar P C, Sproul W D. Vacuum, 1999; 55: 179 [2] Pankov V, Evstigneev M, Prince R H. J Appl Phys, 2002; 92: 4255 [3] Xu J H, Kamiko M, Zhou Y M, Yamamoto R. J Appl Phys, 2001; 89: 3674 [4] Mirkarimi P B, Hultman L, Barnett S A. Appl Phys Lett, 1990; 57: 2654 [5] Chu X, Barnett S A, Wong M S, Sproul W D. Surf Coatings Technol, 1993; 57: 13 [6] Nordina M, Ericsonb F. Thin Solid Films, 2001; 385: 174 [7] Lao J J, Kong M, Zhang H J, Li G Y. Ada Phys Sin, 2004; 53: 1961 (劳技军,孔明,张惠娟,李戈扬.物理学报,2004;53:1961) [8] Wei L, Mei H, Shao N, Kong M, Li G, Li J. Appl Phys Lett, 2005; 86: 21919 [9] Pankov V, Evstigneev M, Prince R H. J Appl Phys, 2002; 92: 4255 [10] Boutos V T, Sanjines R, Karimi A. Surf Coat Technol, 2004; 188: 409 [11] Pharr G M, Oliver W C, Brotzen F R. J Mater Res, 1992; 7: 613 [12] Kato M, Moti T, Schwartz L H. Acta Metall, 1980; 28: 285 [13] Xu J H, Li G Y, Gu M Y. Acta Metall Sin, 1999; 35: 1214 (许俊华,李戈扬,顾明元.金属学报, 1999;35:1214)q |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|