| 不锈钢在扭转/拉伸复合载荷下近门槛值的疲劳裂纹扩展行为 |
| 于慧臣;孙燕国;张岩基;谢世殊;田中启介 |
| 北京航空材料研究院 |
|
| Near Threshold Fatigue Crack Propagation Under Combined Torsion And Tension In Stainless Steel |
| HuiChen Yu |
| 北京航空材料研究院 |
引用本文:
于慧臣; 孙燕国; 张岩基; 谢世殊; 田中启介 . 不锈钢在扭转/拉伸复合载荷下近门槛值的疲劳裂纹扩展行为[J]. 金属学报, 2006, 42(2): 186-190 .
,
,
,
,
.
Near Threshold Fatigue Crack Propagation Under Combined Torsion And Tension In Stainless Steel[J]. Acta Metall Sin, 2006, 42(2): 186-190 .
[1] Pook L P. Int J Fatigue, 1985; 7: 21 [2] Yates J R, Miller K J. Fatigue Fract Eng Mater Struct, 1989; 12: 259 [3] Yoshioka S, Watanabe K, Kitagawa H, Inoue A, Kumasawa M. Trans Jpn Soc Mech Eng, 1984; 50: 1267 [4] Tschegg E K. Mater Sci Eng, 1982; 54: 127 [5] Tschegg E K. J Mater Sci, 1983; 18: 1604 [6] Yu H C, Tanaka K, Akiniwa Y. Fatigue Fract Eng Mater Struct, 1998; 21: 1067 [7] Yu H C, Zhang Y J, Xie S S, Tanaka K. Acta Metall Sin, 2005; 41: 721(于慧臣,张岩基,谢世殊,田中启介.金属学报,2005;41:7211 [8] Yu H C, Tanaka K, Akiniwa Y. In: Senoo M, Xu B Y, Tokuda M, Bundara B, eds., Proc 3rd Int Symp on Microstructures and Mechanical Properties of New Engineering Materials (IMMM'97), Tsu, Japan: Mie University Press, 1997: 309 [9] Ritchie R O, McClintock F A, Hayeb-Hashemi H, Ritter M A. Metall Trans, 1982; 13A: 101 [10] Yu H C, Sun Y G, Xie S S, Tanaka K. Acta Metall Sin, 2005; 41: 73(于慧臣,孙燕国,谢世殊,田中启介.金属学报,2005;41:73) [11] Tada H, Paris P C, Irwin G R. The Stress Intensity Factor Handbook. 2nd ed, Hellertown, Philadelphia: Del Research Corporation, 1985; 27: 3 [12] Rice J R. ASTM STP 415, 1967: 247 [13] Brown M W, Hay E, Miller K J. Fatigue Fract Eng Mater Struct, 1985; 8: 243 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|