| 半固态A356铝合金的稳态流变性能 |
| 张艳菊;毛卫民;赵振铎;刘政 |
| 北京科技大学材料科学与工程学院 |
|
| Rheological Behavior of Semi--solid A356 Aluminum Alloy at Steady State |
| Zhang Yanju |
| 北京科技大学材料科学与工程学院 |
引用本文:
张艳菊; 毛卫民; 赵振铎; 刘政 . 半固态A356铝合金的稳态流变性能[J]. 金属学报, 2006, 42(2): 163-166 .
,
,
,
.
Rheological Behavior of Semi--solid A356 Aluminum Alloy at Steady State[J]. Acta Metall Sin, 2006, 42(2): 163-166 .
[1] Flemings M C. Metall Trans, 1991; A22: 957 [2] Kirkwood D H. Int Mater Rev, 1994; 39: 173 [3] Fan Z. Int Mater Rev, 1994; 47: 49 [4] Spencer D B, Mehrabian R, Flemings M C. Metall Trans, 1972; 3: 1925 [5] Joly P A, Mehrabian R. J Mater Sci, 1976; 11: 1393 [6] Kattamis T Z, Piccone T J. Mater Sci Eng, 1991; A131: 265 [7] Zhen Z S, Mao W M, Yan S J, Zhao A M, Cui C L, Zhong X Y. Acta Metall Sin (Engl Lett), 2002; 15: 505 [8] Quaak C J, Horsten M G, Kool W H. Mater Sci Eng, 1994; A183: 247 [9] Diewwanit I, Flemings M C. In: Kirkwood D H, Kapranos P, eds., Proc 4th Int Conf on Semi-Solid Processing of Alloys and Composites, UK: Department of Engineering ??Materials, University of Sheffield, 1996: 30 [10] Hirami M, Takebayashi K, Yoshikawa Y, Yamaguchi R. ISIJ Int, 1993; 33: 405 [11] Hirami M, Takebayashi K, Yoshikawa Y. ISIJ Int, 1993; 33: 1182 [12] Wang N, Shu G J, Yang H G. Mater Trans JIM, 1990; 31: 715 [13] Yurko J A, de Figueredo A M, Flemings M C. In: Chiarmetta G L, Rosso M eds., Proc 6th Int Conf on Semi—Solid Processing of Alloys and Composites, Turin, Italy: Materials Science and Chemical Engineering Department, Politecnico DI Torino, 2000: 681 [14] Tonmukayakul N, Nguyen Q D, Figueredo A M, Pan Q Y. In: Tsutsui Y, Kiuchi M, Ichikawa K, eds., Proc 7th Int Conf on Semi-Solid Processing of Alloys and Composites, Tsukuba, Japan: National Institute of Advanced Industrial Science and Technology, Japan Society for Technology of Plasticity, 2002: 437 [15] Chen J Y, Fan Z. Mater Sci Technol, 2002; 18: 237 [16] Zhen Z S, Mao W M, Yan S J, Cui C L, Zhao A M, Zhong X Y. Acta Metal Sin, 2003; 39: 71(甄子胜,毛卫民,闫时建,崔成林,赵爱民,钟雪友.金属学报,2003;39:71) [17] Yang X J. PhD Thesis. Shanghai University, 1999(杨湘杰.上海大学博士学位论文,1999) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|