| 利用XPS及电化学方法研究电镀Cr添加剂的作用机理 |
| 关山 张琦 |
| 北京航空航天大学材料科学与工程系;北京 100083 |
|
引用本文:
关山; 张琦 . 利用XPS及电化学方法研究电镀Cr添加剂的作用机理[J]. 金属学报, 2000, 36(11): 1179-1182 .
[1] Serb E J Jr. US Pat 3 505 183, 1970 [2] Chessin H, Newby K. US Pat 4 206 019, 1980 [3] Chessin H, Newby K. US Pat 4 588 481, 1986 [4] Baranyi A D. US Pat 4 406 756, 1983 [5] Laitinen H A. US Pat 4 690 735, 1987 [6] Guan S, Zhang Q, Hu R N. Corros Sci Prot Technol, 2000;in press(关山,张琦,胡如南.腐蚀科学与防护技术,2000;已接收) [7] Briggs D, Seah M P. Practical Surface Analysis byAnger and X-Ray Photoelectron Spectroscopy. Cincinnati: Gardner Publications Inc, 1983: 285 [8] Bockris J O'M. Modern Electrochemistry. Vol.2, NewYork: Plenum Press, 1977: 340 |
|