| 燃烧合成-热压制备A12O3-Tic-ZrO2纳米复合陶瓷的力学性能与显微结构 |
| 董倩 唐清 李文超 |
| 北京科技大学物理化学系;北京100083 |
|
引用本文:
董倩; 唐清; 李文超 . 燃烧合成-热压制备A12O3-Tic-ZrO2纳米复合陶瓷的力学性能与显微结构[J]. 金属学报, 2001, 37(12): 1285-1288 .
[1] Arellano-Lopez A R, Smirnov B I, Goretta K C, RoutbortJ L. Mater Sci Eng, 1998; 252A: 93 [2] Smirnov B I, Nikolaev V I, Orlova T S, Shpeizman V V,Arellano-Lopez A R, Goretta K C, Singh D, Routbort J L.Mater Sci Eng,1998;242A:292 [3]Huang R Z,Tan S H,Jiang D L.J Chin Ceramic Soc, 1993; 21: 349(黄仁政,谭寿洪,江东亮 硅酸盐学报,1993;21:349) [4] Han J C, Wu R J. J Chin Ceramic Soc, 1991; 19: 537(韩杰才,吴忍肼 硅酸盐学报,1991;19:537) [5] Li F Z, Ao Q, Liu Y C, Liu Y X, Tian X J. Mater MechanEng, 1996; 20: 27(李凤照,敖 青,刘援朝,刘玉先,田学洁.机械工程材料,1996;20:27) [6] Tang Q. Ph D Dissertation, Beijing: University of Scienceand Technology Beijing, 1993: 106(唐 清 北京:北京科技大学博士学位沦文,1993:106) [7] Mao D S, Liu X H, Li J, Guo S Y, Zhang X B, Mao Z Y.J Mater Sci, 1998; 33: 5677 [8] Li J, Mao D S, Huang L P. Acta Metall Sin, 1998; 34: 332(郦 剑,茅东升,黄莉萍,金属学报,1998;34:332) [9] Zeng Z Q, Hu X Q, Lin X P, Mao H Z. J Chin CeramicSoc, 1998; 26: 178(曾照强,胡晓清,林旭平,苗赫旺 硅酸盐学报,1998;26:178) [10] Xu L H ,Fang Z H,Shen Z J, Ding Z S,Chin Ceramic Bull,1995;14:12(徐利华,方中华,沈志坚,丁子上,硅酸盐通报,1995,14:12) [11] Yin L W, Li F Z, Liu Y C. Mater Mechan Eng, 1997; 21:35( 尹龙卫,李凤照,刘援朝 机械工程材料,1997;21:35) [12] Niihara K. J Ceram Soc Jpn, 1991; 99: 974 [13] Wang H Z, Gao L, Guo J K.J Chin Ceramic Soc, 1999;27: 1(王宏志,高 濂,郭景坤 硅酸盐学报,1999;27:1) [14] Merzhanov A G. J Self-propagating High-TemperatureSynthesis, 1997; 6: 119 [15] Cutler R A, Rigtrup K M, Virkar A V. J Am Ceram Soc,1992; 75: 36 [16] Zeng H M. Essentials of Advanced Materials for HighTechnolopy, Beijing: China Science and Technology Press,1993: 237(曾汉民.高技术新材料要览,北京:中国科学技术出版社,1993:237) [17] American ceramic society INC. Ceramic Source, 1990; 5:315 [18] Gao J H, Shen Z J, Ding Z S. Acta Mater Compos Sin,1994; 11: 1(高家化,沈志坚,丁子上 复合材料学报,1994;11:1)A |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|