| Fe-Al系金属间化合物中的微观缺陷和电子密度 |
| 邓文 熊良钺 王淑荷 郭建亭 |
| 广西大学物理系;南宁530004 |
|
引用本文:
邓文; 熊良钺; 王淑荷; 郭建亭 . Fe-Al系金属间化合物中的微观缺陷和电子密度[J]. 金属学报, 2002, 38(5): 453-457 .
[1] Mendiratta M G, Ehlers S K, Dimiduk D M, Kerr W R, Mazdiyasni S, Lipsitt H A. In: Stoloff N S, Koch C C, Liu C T, Izumi O eds, High-Temperature Ordered Intermetal-lic Alloys II, Pittsburgh, PA: MRS, 1987; 81: 393 [2]Marcincowski M J, Taylor M E, Kayser F X. J Mater Sci. 1975; 10: 406 [3]Crowford R C, Ray I L. Philos Mag, 1977; 35: 549 [4] Fu C L, Ye Y Y, Yoo M H, Ho K M. Phys Rev B, 1993; 48: 6712 [5] Vedula K, Stephens J R. In: Stoloff N S, Koch C C, Liu C T, Izumi O eds, High-Temperature Ordered Intermetallic Alloys, Pittsburgh, PA: MRS, 1987; 81: 381 [6] Guo J T, Sun C, Tan M H, Li H, Lai W H. Acta Metall Sin ( English Lett), 1990; 3: 249 [7] McKamey C G. Horton J A, Liu C T. Scr Metall, 1988; 22: 1679 [8]Kim S M, Morris D G. Ada. Mater, 1998; 46: 2587 [9]Fu C L, Yoo M H. Mater Res Soc Symp Proc, 1991; 213:667 [10]Bornsen N, Bester G, Meyer B, Fahnle M. J Alloys Compo,2000; 308:1 [11]Deng W, Xiong L Y, Long Q W, Wang S H, Guo J T. Acta Metall Sin( English Lett), 1992; 6:125 [12]Deng W, Xiong L Y, Wang S H, Guo J T, Long Q W. Chin Sci Bulletin ( English Edition), 1997; 42: 1783 [13]Kirkegaard P, Eldrup M.Comput Phys Commun, 1974;7: 401 [14]Brandt W, Reinheimer J. Phys Rev B, 1970; 2: 3104 [15]Brandt W, Dupasquier A. Positron Solid-State Physics. Amsterdam: Holland Publish Co, 1983: 200 [16] Shirai Y, Schaefer H E, Seeger A. In:Dorikens-Vanpraet L, Dorikens M, Segers D eds, Positron Annihilation, Sin gapore, New Jersey, Hong Kong:ICPA-8, 1988: 419 [17]Wurschum R,Grupp C,Schaefer H E. Phys Rev Lett, 1995; 75 (1): 97 [18] Dupasquier A. Mills A. P. Positron Spectroscopy of Solids. Amsterdam: IOS Press, 1995: 514 [19] Brandt W, Paulin R. Phys Rev B, 1972; 5:2430 [20]Lock D G, West R N. J Phys F(Met Phys), 1974; 4: 2179 [21]Stott M J, Kubica P. Phys Rev B, 1975; 11: 1 [22]Yang W Y, Sheng L Z, Sun Z Q, Huang Y D, Mao W M, Zhang B S, Ye C T. Acta Metall Sin, 1996; 32: 799 (杨王(?),盛丽珍.孙祖庆,黄原定.毛卫民.张百生.叶春 堂.金属学报,1996;32:799)! |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|