| 水热法合成负热膨胀材料ZrW2O8 |
| 邢奇凤;邢献然;杜 凌;于然波;陈 骏;邓金侠;罗 君 |
| 北京科技大学物理化学系; 北京 100083; 北京科技大学化学系; 北京 100083 |
|
| Hydrothermal Synthesis of Negative Thermal Expansion Material ZrW2O8 |
| XING Qifeng; XING Xianran; DU Ling; YU Ranbo; CHEN Jun; DENG Jinxia; LUO Jun |
| Department of Physical Chemistry; University of Science & Technology Beijing; Beijing 100083; Department of Chemistry; University of Science & Technology Beijing; Beijing 100083 |
引用本文:
邢奇凤; 邢献然; 杜凌; 于然波; 陈骏; 邓金侠; 罗君 . 水热法合成负热膨胀材料ZrW2O8[J]. 金属学报, 2005, 41(6): 669-672 .
,
,
,
,
,
,
.
Hydrothermal Synthesis of Negative Thermal Expansion Material ZrW2O8[J]. Acta Metall Sin, 2005, 41(6): 669-672 .
[1]Mary T A,Evans J S O,Vogt T,Sleight A W.Science,1996;272:90 [2]Evans J S O,Hu Z,Jorgensen J D,Argyriou D N,Short S,Sleight A W.Science,1997;275:61 [3]Zhao X H.Chin Chem Bull,1998;(11):19 (赵新华.化学通报,1998;(11):19) [4]Wang C,Wang T M,Shen R,Liang J K.Physics,2001;30:772 (王聪,王天民,沈容,梁敬魁.物理,2001;30:772) [5]Li S H,Zhao X H.Rare Met Cemented Carbides,2002;30(1):14 (李淑欢,赵新华.稀有金属与硬质合金,2002;30(1):14) [6]Nakajima N,Yamamura Y,Tsuji T.Solid State Commun,2003;128:193 [7]Holzer H,Dunand D C.J Mater Res,1999;14:780 [8]Verdon C,Dunand D C.Scr Mater,1997;36:1075 [9]Shen R,Wang C,Wang T M.J Inorg Mater,2002;17:1089 (沈容,王聪,王天民.无机材料学报,2002;17:1089) [10]Chang L L Y,Scroger M G,Phillips B.J Am Ceram Soc,1967;50:211 [11]Khosrovani N,Sleight A W,Vogt T.J Solid State Chem,1997;132:355 [12]Kameswari U,Sleight A W,Evans J S O.Int J Inorg Mater,2000;2:333 [13]Shen R,Wang T M,Bai H L,Xiong C J.Mater Eng,2003;(3):3 (沈容,王天民,白海龙,熊常健.材料工程,2003;(3):3) [14]Closmann C,Sleight A W.J Solid State Chem,1998;139:424 [15]Wilkinson A P,Lind C,Pattanaik S.Chem Mater,1999;11:101 [16]Kong X Y,Wu J S,Zeng Z P.J Chin Ceram Soc,1999;27:265 (孔向阳,吴建生,曾振鹏.硅酸盐学报,1999;27:265) [17]Evans J S O,Mary T A,Vogt T,Subramanian A,Sleight A W.Chem Mater,1996;8:2809 [18]Gallardo-Amores J M,Amador U,Moran E,Alario- Pranco M A.Int J Inorg Mater,2000;2:123a |
|