| Co41Ni32Al27-xSix合金的马氏体相变和磁性转变 |
| 罗丰华 及川胜成 石田清仁 |
| 中南大学粉末冶金国家重点实验室; 长沙 410083 |
|
| Martensitic Transformation and Magnetic Transition of Co41Ni32Al27-xSix Alloy |
| LUO Fenghua; OIKAWA Katsunari; ISHIDA Kiyohito |
| State Key Laboratory for Powder Metallurgy; Central South University; Changsha 410083 |
引用本文:
罗丰华; 及川胜成; 石田清仁 . Co41Ni32Al27-xSix合金的马氏体相变和磁性转变[J]. 金属学报, 2005, 41(7): 680-684 .
,
,
.
Martensitic Transformation and Magnetic Transition of Co41Ni32Al27-xSix Alloy[J]. Acta Metall Sin, 2005, 41(7): 680-684 .
[1] Ullakko K, Huang J K, Kanter C, Kokorin V V, O'Handley R C. Appl Phys Lett, 1996; 69: 1966 [2] Murray S J, Marioni M, Kukla A, Robinson J, O'Handley R C, Allem S M. J Appl Phys, 2000; 87: 5774 [3] Murray S J, Marioni M, Allen S M, O'Handley R C. Appl Phys Lett, 2000; 77: 886 [4] Gejima F, Sutou Y, Kainuma R, Ishida K. Metall Mater Trans, 1999; 30A: 2721 [5] Kainuma R, Gejima F, Sutou Y, Ohnuma Y, Ishida K. Mater Trans JIM, 2000; 41: 943 [6] Fujita A, Fukamichi K, Gejima F, Kainuma R, Ishida K. Appl Phys Lett, 2000; 77: 3054 [7] James R D, Wuttig M. Philos Mag, 1998; 77A: 1273 [8] Furuya Y, Hangood N W, Kimura H, Watanabe T. Mater Trans JIM, 1998; 39: 1248 [9] Kakeshita T, Takeuchi T, Fukuda T, Saburi T, Oshima R, Muto S, Kishio K. Mater Trans JIM, 2000; 41: 882 [10] Oikawa K, Ota T, Gejima F, Ohmori T, Kainuma R, Ishida K. Mater Trans JIM, 2001; 42: 2472 [11] Wuttig M, Li J, Craciunescu C. Scr Mater, 2001; 44: 2393 [12] Oikawa K, Ota T, Ohmori T, Tanaka Y, Morito H, Fujita A, Kainuma R, Fukamichi K, Ishida K. Appl Phys Lett, 2002; 81: 5201 [13] Liu Z H, Zhang M, Cui Y T, Zhou Y Q, Wang W H, Wu G H, Zhang X X, Xiao G. Appl Phys Lett, 2003; 82: 424 [14] Kainuma R, Ise M, Jia C C, Ohtani H, Ishida K. Intermetallics, 1996; 4: S151 [15] Karaca H E, Karaman I, Lagoudas D C, Maier H J, Chumlyakov Y I. Scr Mater, 2003; 49: 831 [16] Oikawa K, Wulff L, lijima T, Gejima F, Ohmori T, Fujita A, Fukamichi K, Kainuma R, Ishida K. Appl Phys Lett, 2001; 79: 3290 [17] Fujita A, Morito H, Kudo T, Fukamichi K, Kainuma R, Ishida K, Oikawa K. Mater Trans JIM, 2003; 44: 2180 [18] Morito H, Fujita A, Fukamichi K, Kainuma R, Ishida K. Appl Phys Lett, 2002; 81: 1657 [19] Murakami Y, Shindo D, Oikawa K, Kainuma R, Ishida K. Ada Mater, 2002; 50: 2173 [20] Tanaka Y, Ohmori T, Oikawa K, Kainuma R, Ishida K. Mater Trans JIM, 2004; 45: 427 [21] Liang Y, Sutou Y, Wada T, Lee G, Taya M, Mori T. Scr Mater, 2003; 48: 1415 [22] Lefebvre F, Mentzen B F, Bosselet F, Viala J C. Colloids Surfaces, 1999; 158A: 121 [23] Oikawa K, Ota T, Sutou Y, Ohmori T, Kainuma R, Ishida K. Mater Trans JIM, 2000; 43: 2360 [24] Wutting M, Liu L, Tsuchiya K, James R D. J Appl Phys, 2000; 87: 4707 [25] Hames F A. J Appl Phys, 1960; 31: 370S |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|