| A--TIG焊中氧含量对熔池流动方式影响的数值模拟 |
| 赵玉珍 雷永平 史耀武 |
| 北京工业大学材料学院; 北京 100022 |
|
| Modeling of the Effects of Oxygen Content on Flow Patterns in A-Tig Welding |
| ZHAO Yuzhen; LEI Yongping; SHI Yaowu |
| School of Materials Science and Engineering; Beijing University of Technology; Beijing 100022 |
引用本文:
赵玉珍; 雷永平; 史耀武 . A--TIG焊中氧含量对熔池流动方式影响的数值模拟[J]. 金属学报, 2004, 40(10): 1085-1092 .
,
,
.
Modeling of the Effects of Oxygen Content on Flow Patterns in A-Tig Welding[J]. Acta Metall Sin, 2004, 40(10): 1085-1092 .
[1] Paskell T. Weld J, 1997; 4: 57 [2] Lucas W. Weld Met Fabr, 1996; 1: 11 [3] Anderson P C J. Weld Met Fabr, 1996; 3: 108 [4] Yang C L, Ushio M. Welding, 2000; 4: 16(杨春利,Ushio M.焊接,2000;4:16) [5] Yang C L, Ushio M. Welding, 2000; 5: 15(杨春利,Ushio M.焊接,2000;5:15) [6] Heiple C R, Roper J R. Weld J, 1982; 61(4) : 97 [7] Heiple C R, Roper J R. Weld J, 1983; 62(3) : 72 [8] Heiple C R, Roper J R. Weld J, 1981; 60(8) : 143 [9] Kou S, Sun D K. Metall Trans A, 1985; 16A(2) : 203 [10] Tsai N S, Eagar T W. Metall Trans B, 1985; 16B: 841 [11] Zacharia T, David S A. Weld J, 1989; 12: 499 [12] Zacharia T, David S A. Weld J, 1989; 12: 510 [13] Pitscheneder W, Debroy T, Mundra K, Ebner R. Weld J, 1996; 3: 71 [14] Wang Y, Shi Q, Tsai H L. Metall Trans B, 2001; 32B(2) :145 [15] Wang Y, Tsai H L. Metall Trans B, 2001; 32B(6) : 501 [16] Aidun D K, Martin S A. J Mater Eng Per/or, 1997; 6:496 [17] Bennon W D, Incropera F P. Int J Heat Mass Trans, 1987;30: 2161 [18] Sahoo P, Debroy T, Mcnallan M J. Metall Trans B, 1998;19B: 483 [19] Lu S P. Mater Trans, 2002; 11: 2926 [20] Hsieh R I, Pan Y T, Liou H Y. J Mater Eng Perfor, 1999;8(1) : 68 [21] Yang C L, Ushio M. Chin J Mech Eng, 2000; 10: 59(杨春利,Ushio M.机械工程学报,2000;10:59) [22] Liu F Y, Lin S B, Yang C L. Trans China Weld Inst, 2002; 23(2) : 5(刘风尧,林三宝.焊接学报,2002;23(2) :5) [23] Zhang R H, Fan D. J Gansu Univ Technol, 2002; 28(1) : 7(张瑞华,樊丁.甘肃工业大学学报,2002;28(1) :7) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|