| 疲劳态铜单晶高速形变下绝热剪切带的形成 |
| 李军伟 李明扬 郭小龙 李守新 |
| 中国科学院金属研究所沈阳材料科学国家(联合)实验室; 沈阳 110016 |
|
引用本文:
李军伟; 李明扬; 郭小龙; 李守新 . 疲劳态铜单晶高速形变下绝热剪切带的形成[J]. 金属学报, 2005, 41(2): 161-166 .
[1] Nemat-Nasser S, Li Y L. Acta Mater, 1998; 46: 565 [2] Kiritani M, Satoh Y, Kizuka Y, Arakaua K. Philos MagLett, 1999; 79: 797 [3] Sanchez J C, Murr L E, Staudhammer K P. Acta Mater,1997; 45: 3223 [4] Glenn T, Bradley W. Metall Trans, 1973; 4: 1923 [5] Gourdin W H, Lassila D H. Acta Metall Mater, 1991; 39:2337 [6] Nai-Yong, Niessen P, Pick R J. Mater Sci Eng, 1991;A131: 153 [7] Audrade U, Meyers M A, Vecchid K S, Chokshi A H. ActaMatall Mater, 1994; 42: 3183 [8] Edington J W. Philos Mag, 1969; 19: 1189 [9] Rashid M M, Gray G T, Nemat-Nasser S. Philos Mag A,1992; 65: 707 [10] Cheng G Q, Li S X. Journal of Ballistics, in press(程国强,李守新.弹道学报,待发表) [11] Winter A T. Philos Mag, 1974; 29: 719 [12] Li S X, Li Y, Li G Y, Yang J H, Wang Z G, Lu K. PhilosMag A, 2002; 82: 867 [13] Li S X, Li X W, Zhang Z F, Lu K. Philos Mag A, 2002;82: 3129 [14] Wright T W, Ockendon H. Int J Plast, 1996; 12: 927 [15] Chang Y W, Asaro R J. Acta Metall, 1982; 30: 241 [16] Peirce D, Asaro R J. Acta Metall, 1982; 30: 1087 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|