O点阵模型及其在界面位错计算中的应用 |
张文征 |
清华大学材料科学与工程系;北京100084 |
|
引用本文:
张文征 . O点阵模型及其在界面位错计算中的应用[J]. 金属学报, 2002, 38(8): 785-794 .
[1] Sutton A P, Balluffi R W. Interfaces in Crystalline Materials. Oxford: Oxford University Press, 1995 [2] Howe J M. Interfaces in Materials. New York: John Wiley and Sons, 1997 [3] Smith D A, Shiflet G. Mater Sci Eng, 1987; 86: 67 [4] Ping D H, Li D X, Huang J Y, He L L.In: Ye H Q et al eds., Structures and Characteristics of Interfaces in Materials, Beijing: Science Press, 1999: 641999: 64) [5] Porter D A, Easterling K E.Phase Transformations inMetals and Alloys. New York: Chapman & Hall, 1992 [6] Feng D. In: Peng D et al eds., Metal Physics, Beijing:Science Press, 1987: 375 [7] Song Y J. Grian Boundaries and Strength of Metals.Xi'an: Xi'an Jiaotong University Press, 1987(宋余九.金属的晶界与强度.西安:西安交大出版社,1987) [8] Yu Y N. Principles of Physical Metallurgy. Beijing: Metallurgy Industry Press, 2000 [9] Bollmann W. Crystal Defects and Crystalline Interfaces.Berlin: Springer, 1970 [10] Bollmann W.Crystal Lattices,Interfaces,Matrices.Geneva: Bollmann, 1982 [11] Ralph B, Randle V. In: Lorimer G W ed., Phase Trans-formations' 87, London: Institute of Metals, 1988: 613 [12] Lin D L. In: Li H D, Xiao J M eds., Surface and In-terfaces in Materials, Beijing: Tsinghua University Press,1990: 165(林栋梁.见:李恒德,肖纪美主编,材料表面与界面,北京:清华大学出版社,1990:165) [13] Luo C P, Liu Z Y. In: Li H D, Xiao J M eds., Surface and Interfaces in Materials, Beijing: Tsinghua University Press, 1990: 201(罗承萍,刘正义.见:李恒德,肖纪美主编,材料表面与界面.北京:清华大学出版社,1990:201) [14] Christian J W. The Theory of Transformation in Metalsand Alloys. Oxford: Pergamon Press, 1975 [15] Smith D A, Pond R C. Int Metall Rev, 1976; 11: 61 [16] Knowles K M, Philos Mag, 1982; 46A: 951 [17] Hirth J P, Lothe J. Theory of Dislocations. 2nd ed., Malabar: Krieger, 1992 [18] Bollmann W, Nissen H U. Acta Crystallogr, 1968; 24A:546 [19] Hall M G, Rigsbee J M, Aaronson H I. Acta Metall, 1986;34: 1419 [20] Zhang W-Z, Purdy G R. Philos Mag, 1993; 68A: 279 [21] Zhang W-Z, Weatherly G C. Submitted to Progr MateiSci [22] Wayman C M. Introduction to the Crystallography ofMartensitic Transformations.New York: MacMillan,1964 [23] Zhang W-Z, Purdy G R. Philos Mag, 1993; 68A: 291 [24] Zhang W-Z. Submitted to Philos Mag [25] Weatherly G C, Zhang W Z. Metall Mater Trans, 1994;25A: 1865 [26] Luo C P, Dahmen U. Acta Mater, 1998; 46: 2063 [27] Zhang W-Z. Philos Mag, 1998; 78A: 913{ |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|