金属学报  2002, Vol. 38 Issue (8): 785-794     
  论文 本期目录 | 过刊浏览 |
O点阵模型及其在界面位错计算中的应用
张文征
清华大学材料科学与工程系;北京100084
引用本文:

张文征 . O点阵模型及其在界面位错计算中的应用[J]. 金属学报, 2002, 38(8): 785-794 .

全文: PDF(476 KB)  
摘要: 介绍了描述O点阵特征的基本参量:主O点阵基矢、主O点阵面和O胞壁的定义和计算公式.提供了一般界面上周期位错结构的矩阵方法和计算特殊界面位错结构的简易矢量方法.还分析了O点阵描述界面位错的条件和局限,讨论了一般界面和大错配界面上位错结构的计算.
关键词 : 界面位错结构,  O点阵界面模型,  惯习面    
Key words:
收稿日期: 2001-12-13     
ZTFLH:  O71  
[1] Sutton A P, Balluffi R W. Interfaces in Crystalline Materials. Oxford: Oxford University Press, 1995
[2] Howe J M. Interfaces in Materials. New York: John Wiley and Sons, 1997
[3] Smith D A, Shiflet G. Mater Sci Eng, 1987; 86: 67
[4] Ping D H, Li D X, Huang J Y, He L L.In: Ye H Q et al eds., Structures and Characteristics of Interfaces in Materials, Beijing: Science Press, 1999: 641999: 64)
[5] Porter D A, Easterling K E.Phase Transformations inMetals and Alloys. New York: Chapman & Hall, 1992
[6] Feng D. In: Peng D et al eds., Metal Physics, Beijing:Science Press, 1987: 375
[7] Song Y J. Grian Boundaries and Strength of Metals.Xi'an: Xi'an Jiaotong University Press, 1987(宋余九.金属的晶界与强度.西安:西安交大出版社,1987)
[8] Yu Y N. Principles of Physical Metallurgy. Beijing: Metallurgy Industry Press, 2000
[9] Bollmann W. Crystal Defects and Crystalline Interfaces.Berlin: Springer, 1970
[10] Bollmann W.Crystal Lattices,Interfaces,Matrices.Geneva: Bollmann, 1982
[11] Ralph B, Randle V. In: Lorimer G W ed., Phase Trans-formations' 87, London: Institute of Metals, 1988: 613
[12] Lin D L. In: Li H D, Xiao J M eds., Surface and In-terfaces in Materials, Beijing: Tsinghua University Press,1990: 165(林栋梁.见:李恒德,肖纪美主编,材料表面与界面,北京:清华大学出版社,1990:165)
[13] Luo C P, Liu Z Y. In: Li H D, Xiao J M eds., Surface and Interfaces in Materials, Beijing: Tsinghua University Press, 1990: 201(罗承萍,刘正义.见:李恒德,肖纪美主编,材料表面与界面.北京:清华大学出版社,1990:201)
[14] Christian J W. The Theory of Transformation in Metalsand Alloys. Oxford: Pergamon Press, 1975
[15] Smith D A, Pond R C. Int Metall Rev, 1976; 11: 61
[16] Knowles K M, Philos Mag, 1982; 46A: 951
[17] Hirth J P, Lothe J. Theory of Dislocations. 2nd ed., Malabar: Krieger, 1992
[18] Bollmann W, Nissen H U. Acta Crystallogr, 1968; 24A:546
[19] Hall M G, Rigsbee J M, Aaronson H I. Acta Metall, 1986;34: 1419
[20] Zhang W-Z, Purdy G R. Philos Mag, 1993; 68A: 279
[21] Zhang W-Z, Weatherly G C. Submitted to Progr MateiSci
[22] Wayman C M. Introduction to the Crystallography ofMartensitic Transformations.New York: MacMillan,1964
[23] Zhang W-Z, Purdy G R. Philos Mag, 1993; 68A: 291
[24] Zhang W-Z. Submitted to Philos Mag
[25] Weatherly G C, Zhang W Z. Metall Mater Trans, 1994;25A: 1865
[26] Luo C P, Dahmen U. Acta Mater, 1998; 46: 2063
[27] Zhang W-Z. Philos Mag, 1998; 78A: 913{
[1] 顾新福 张文征. 马氏体相变晶体学的简易矢量分析方法[J]. 金属学报, 2011, 47(2): 241-245.
[2] 邱冬; 张文征 . 沉淀相变晶体学模型的研究进展[J]. 金属学报, 2006, 42(4): 341-349 .
[3] 罗承萍;许麟康;查健中. 300M超高强度钢板条马氏体的晶体学研究[J]. 金属学报, 1993, 29(7): 28-33.
[4] 谷南驹;王瑞祥;殷福星. 孪晶马氏体的自协作效应及不变惯习面[J]. 金属学报, 1991, 27(3): 33-40.
[5] 罗承萍;赵方. 4Cr5MoV1Si(H13)钢合金氮化物的形貌和晶体学特征[J]. 金属学报, 1990, 26(6): 34-39.
[6] 刘禹门;伍尚华. 高碳铁合金马氏体的特征[J]. 金属学报, 1988, 24(5): 325-330.