| NiTi合金中一个新的时效析出相 |
| 徐爱群 |
| 东南大学分析测试中心; 南京 210096 |
|
| A New Aging Precipitated Phase in NiTi Alloy |
| XU Aiqun |
| Analysis and Testing Center; Southeast University; Nanjing 210096 |
引用本文:
徐爱群 . NiTi合金中一个新的时效析出相[J]. 金属学报, 2004, 40(2): 125-129 .
.
A New Aging Precipitated Phase in NiTi Alloy[J]. Acta Metall Sin, 2004, 40(2): 125-129 .
[1] Yi H C, Moore J J. J Mater Sci, 1992; 27: 5067 [2] Funakubo K ed., translate by Qian D F. Shape Memory Alloy. Beijing: China Machine Press, 1984: 85(舟久保 熙康编,千冬范译.形状记忆合金.北京:机械工业出版社,1984:85) [3] He Z R. Funct Mater, 1998; 29: 157(贺志荣.功能材料,1998;29:157) [4] He Z R, Zhang Y H, Miyazaki S. Met Heat Treat, 1996; (10) : 7(贺志荣,张永宏,宫崎修一.金属热处理,1996;(10) :7) [5] Nishida M, Wayman C M, Honma T. Metall Trans, 1986; 17A: 1505 [6] Hwang C M, Meichle M, Salamon M B, Wayman C M. Philos Mag, 1983; 47A: 31 [7] The Metallography and Heat Treatment Teaching and Research Group of Beijing Steel College. Metal Heat Treatment. Beijing: China Industry Press, 1961: 135(北京钢铁学院金相及热处理教研组.金属热处理.北京:中国工业出版社,1961:135) |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|