| Mo含量对CrAlMoN涂层微观结构、力学性能及摩擦学性能的影响 |
毕健浩男1, 张艳2, 王振玉2( ), 周晟昊2, 刘永跃3, 张小岩4, 汪爱英2 |
1 浙江工业大学 化学工程学院 杭州 310014 2 中国科学院宁波材料技术与工程研究所 海洋关键材料全国重点实验室 全省极端环境材料表面与界面重点实验室 宁波 315201 3 宁波合力科技股份有限公司 宁波 315799 4 宁波大榭开发区天正模具有限公司 宁波 315812 |
|
| Effect of Mo Content on the Microstructure, Mechanical and Tribological Properties of CrAlMoN Coatings |
BI Jianhaonan1, ZHANG Yan2, WANG Zhenyu2( ), ZHOU Shenghao2, LIU Yongyue3, ZHANG Xiaoyan4, WANG Aiying2 |
1 College of Chemical Engineering, Zhejiang University of Technology, Hangzhou 310014, China 2 State Key Laboratory of Advanced Marine Materials, Zhejiang Key Laboratory of Extreme-environmental Material Surfaces and Interfaces, Ningbo Institute of Materials Technology and Engineering, Chinese Academy of Sciences, Ningbo 315201, China 3 Ningbo Heli Mould Technology Co. Ltd., Ningbo 315799, China 4 Ningbo Tianzheng Mould Co. Ltd., Ningbo 315812, China |
引用本文:
毕健浩男, 张艳, 王振玉, 周晟昊, 刘永跃, 张小岩, 汪爱英. Mo含量对CrAlMoN涂层微观结构、力学性能及摩擦学性能的影响[J]. 金属学报, 2025, 61(9): 1413-1424.
Jianhaonan BI,
Yan ZHANG,
Zhenyu WANG,
Shenghao ZHOU,
Yongyue LIU,
Xiaoyan ZHANG,
Aiying WANG.
Effect of Mo Content on the Microstructure, Mechanical and Tribological Properties of CrAlMoN Coatings[J]. Acta Metall Sin, 2025, 61(9): 1413-1424.
| [1] |
Yang B, Chen L, Chang K K, et al. Thermal and thermo-mechanical properties of Ti-Al-N and Cr-Al-N coatings [J]. Int. J. Refract. Met. Hard Mater., 2012, 35: 235
|
| [2] |
Reiter A E, Mitterer C, de Figueiredo M R, et al. Abrasive and adhesive wear behavior of arc-evaporated Al1 - x Cr x N hard coatings [J]. Tribol. Lett., 2010, 37: 605
|
| [3] |
Li W Z, Polcar T, Evaristo M, et al. High temperature properties of the Cr-Nb-Al-N coatings with increasing Al contents [J]. Surf. Coat. Technol., 2013, 228: 187
|
| [4] |
Wang Y X, Tang Y J, Wan W, et al. Effect of Ni doping on the microstructure and toughness of CrAlN coatings deposited by magnetron sputtering [J]. Mater. Res. Express, 2020, 7: 026414
|
| [5] |
Wang C C, Xu B B, Wang Z Y, et al. Tribological mechanism of (Cr, V)N coating in the temperature range of 500-900 oC [J]. Tribol. Int., 2021, 159: 106952
|
| [6] |
Zhang Y P, Wang Z Y, Guo P, et al. Enhanced tribological behavior of VAlN hard ceramic coating with intermittent amorphous carbon layer [J]. Ceram. Int., 2023, 49: 15091
|
| [7] |
Liu C B, Pei W, Huang F, et al. Improved mechanical and thermal properties of CrAlN coatings by Si solid solution [J]. Vacuum, 2016, 125: 180
|
| [8] |
Hollerweger R, Zhou L, Holec D, et al. Controlling microstructure, preferred orientation, and mechanical properties of Cr-Al-N by bombardment and alloying with Ta [J]. J. Appl. Phys., 2016, 119: 065304
|
| [9] |
Qi Z B, Wu Z T, Wang Z C. Improved hardness and oxidation resistance for CrAlN hard coatings with Y addition by magnetron co-sputtering [J]. Surf. Coat. Technol., 2014, 259: 146
|
| [10] |
Tian J L, Hu C, Chen L, et al. Structure, mechanical and thermal properties of Y-doped CrAlN coatings [J]. Trans. Nonferrous Met. Soc. China, 2021, 31: 2740
|
| [11] |
Bobzin K, Brögelmann T, Kalscheuer C. Arc PVD (Cr, Al, Mo)N and (Cr, Al, Cu)N coatings for mobility applications [J]. Surf. Coat. Technol., 2020, 384: 125046
|
| [12] |
Chen L, Liu Z Q, Xu Y X, et al. Influence of Zr on structure, mechanical and thermal properties of Cr-Al-N coatings [J]. Surf. Coat. Technol., 2015, 275: 289
|
| [13] |
Rajput S S, Gangopadhyay S, Yaqub T B, et al. Room and high temperature tribological performance of CrAlN(Ag) coatings: The influence of Ag additions [J]. Surf. Coat. Technol., 2022, 450: 129011
|
| [14] |
Shi J, Chen Y, Liu H, et al. Effect of Mo and C contents on the crystal structure and properties of AlCrN films [J]. China Surf. Eng., 2022, 35(6): 286
|
| [14] |
施 杰, 陈 云, 刘 浩 等. Mo和C含量对AlCrN薄膜组织和性能的影响 [J]. 中国表面工程, 2022, 35(6): 286
|
| [15] |
Wang Y X, Ji Y. Influence of Mo doping on the microstructure, friction, and wear properties of CrAlN films [J]. J. Mater. Eng. Perform., 2021, 30: 1938
|
| [16] |
Sergevnin V S, Blinkov I V, Belov D S, et al. Phase formation in the Ti-Al-Mo-N system during the growth of adaptive wear-resistant coatings by arc PVD [J]. Inorg. Mater., 2016, 52: 735
|
| [17] |
Fu Y Q, Zhou F, Zhang M D, et al. Structural, mechanical and tribocorrosion performances of CrMoSiN coatings with various Mo contents in artificial seawater [J]. Appl. Surf. Sci., 2020, 525: 146629
|
| [18] |
Qi D L, Chen J J, Liu J, et al. Influence of molybdenum addition on oxidation resistance of CrN coatings [J]. Rare Met. Mater. Eng., 2021, 50: 1505
|
| [18] |
齐东丽, 陈建金, 刘 俊 等. 钼添加对CrN涂层抗氧化性能的影响(英文) [J]. 稀有金属材料与工程, 2021, 50: 1505
|
| [19] |
Wang Y X, Lou B Y. Microstructure and high-temperature friction and wear properties of CrAlMoN film [J]. Oxid. Met., 2021, 95: 239
|
| [20] |
Fu X J, Li R C, Li Y, et al. Tribological properties of CrN and CrAlN coatings in the presence of organic molybdenum additives [J]. China Surf. Eng., 2021, 34(6): 181
|
| [20] |
付小静, 李瑞川, 李 阳 等. 有机钼添加剂作用下CrN和CrAlN涂层的摩擦学性能 [J]. 中国表面工程, 2021, 34(6): 181
|
| [21] |
Zhou D W, Wang Z Y, Zhang Y, et al. Stimulated corrosion damage of Ti-Al-N multilayer coatings under interval salt spray and hot condition [J]. Corros. Sci., 2023, 222: 111431
|
| [22] |
Wang L, Fu Z Q, Yue W, et al. Effect of W content on tribological performance of CrWN coating under dry friction and oil lubrication conditions [J]. Rare Met. Mater. Eng., 2019, 48: 2371
|
| [22] |
王 莉, 付志强, 岳 文 等. W含量对CrWN涂层在干摩擦和油润滑下的摩擦学性能影响 [J]. 稀有金属材料与工程, 2019, 48: 2371
|
| [23] |
Yu G Q, Tay B K, Lau S P, et al. Effects of N ion energy on titanium nitride films deposited by ion assisted filtered cathodic vacuum arc [J]. Chem. Phys. Lett., 2003, 374: 264
|
| [24] |
Wang L, Wang Z Y, Chen R D, et al. Preparation and erosion performance of composite CrN coatings through zigzag structural design [J]. China Surf. Eng., 2023, 36(3): 65
|
| [24] |
王 丽, 王振玉, 陈仁德 等. 复合zigzag结构CrN涂层的设计制备及冲蚀性能 [J]. 中国表面工程, 2023, 36(3): 65
|
| [25] |
Zhou S H, Kuang T C, Qiu Z G, et al. Microstructural origins of high hardness and toughness in cathodic arc evaporated Cr-Al-N coatings [J]. Appl. Surf. Sci., 2019, 493: 1067
|
| [26] |
Zhou S H, Zhao W C, Qiu Z G, et al. Improved load-bearing capacity of Mo-doped Ti-N coatings: Effects of Mo alloying and GB plasticity [J]. Surf. Coat. Technol., 2021, 424: 127630
|
| [27] |
Meindlhumer M, Ziegelwanger T, Zalesak J, et al. Precipitation-based grain boundary design alters inter- to trans-granular fracture in AlCrN thin films [J]. Acta Mater., 2022, 237: 118156
|
| [28] |
Iram S, Wang J M, Cai F, et al. Effect of bilayer number on mechanical and wear behaviours of the AlCrN/AlCrMoN coatings by AIP method [J]. Surf. Eng., 2021, 37: 536
|
| [29] |
Zhang Y, Zhou Y J, Lin J P, et al. Solid-solution phase formation rules for multi-component alloys [J]. Adv. Eng. Mater., 2008, 10: 534
|
| [30] |
Chen Y, Xu Y X, Zhang H Q, et al. Improving high-temperature wear resistance of arc-evaporated AlCrN coatings by Mo alloying [J]. Surf. Coat. Technol., 2023, 456: 129253
|
| [31] |
Fan Q X, Zhang J J, Wu Z H, et al. Influence of Al content on the microstructure and properties of the CrAlN coatings deposited by arc ion plating [J]. Acta Metall. Sin. (Engl. Lett.), 2017, 30: 1221
|
| [32] |
Lu C, Jia J H, Fu Y Y, et al. Influence of Mo contents on the tribological properties of CrMoN/MoS2 coatings at 25-700 oC [J]. Surf. Coat. Technol., 2019, 378: 125072
|
| [33] |
Zhang S, Sun D E, Fu Y Q, et al. Toughness measurement of thin films: A critical review [J]. Surf. Coat. Technol., 2005, 198: 74
|
| [34] |
Perfilyev V, Moshkovich A, Lapsker I, et al. The effect of vanadium content and temperature on stick-slip phenomena under friction of CrV(x)N coatings [J]. Wear, 2013, 307: 44
|
| [35] |
Sergevnin V S, Blinkov I V, Volkhonskii A O, et al. Structure formation of adaptive arc-PVD Ti-Al-Mo-N and Ti-Al-Mo-Ni-N coatings and their wear-resistance under various friction conditions [J]. Surf. Coat. Technol., 2019, 376: 38
|
| [36] |
Camacho-López M A, Escobar-Alarcón L, Picquart M, et al. Micro-Raman study of the m-MoO2 to α-MoO3 transformation induced by cw-laser irradiation [J]. Opt. Mater., 2011, 33: 480
|
| [37] |
Xu B B, Guo P, Wang Z Y, et al. Anti-wear Cr-V-N coating via V solid solution: Microstructure, mechanical and tribological properties [J]. Surf. Coat. Technol., 2020, 397: 126048
|
| [38] |
Iram S, Cai F, Wang J M, et al. Effect of addition of Mo or V on the structure and cutting performance of AlCrN-based coatings [J]. Coatings, 2020, 10: 298
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|