金属学报  2024, Vol. 60 Issue (6): 731-742    DOI: 10.11900/0412.1961.2023.00498
  综述 本期目录 | 过刊浏览 |
Ni-Cr合金在富CO2 气氛中的高温腐蚀研究进展
谢云1(), Zhang Jianqiang2, 彭晓1
1 南昌航空大学 材料科学与工程学院 南昌 330063
2 School of Materials Science and Engineering, University of New South Wales, Sydney 2052, Australia
Research Advances in High Temperature Corrosion of Ni-Cr Alloys in CO2-Rich Environments
XIE Yun1(), Zhang Jianqiang2, PENG Xiao1
1 School of Materials Science and Engineering, Nanchang Hangkong University, Nanchang 330063, China
2 School of Materials Science and Engineering, University of New South Wales, Sydney 2052, Australia
引用本文:

谢云, Zhang Jianqiang, 彭晓. Ni-Cr合金在富CO2 气氛中的高温腐蚀研究进展[J]. 金属学报, 2024, 60(6): 731-742.
Yun XIE, Jianqiang Zhang, Xiao PENG. Research Advances in High Temperature Corrosion of Ni-Cr Alloys in CO2-Rich Environments[J]. Acta Metall Sin, 2024, 60(6): 731-742.

全文: PDF(1930 KB)   HTML
摘要: 

发展富氧燃烧技术和提高锅炉的蒸汽参数可以有效减少燃煤电厂的CO2排放,有助于火力发电行业实现“碳达峰-碳中和”的目标,但采用上述技术对锅炉材料的抗CO2高温腐蚀性能和高温蠕变强度提出了更高要求,镍基合金有望成为优选材料。针对先进超超临界发电机组富氧燃烧烟气高含CO2的特点,本文综述了目前关于Ni-Cr合金在富CO2气氛中的高温腐蚀研究成果,重点介绍了CO2气氛对Ni-Cr合金热生长Cr2O3保护膜的影响,阐明了Ni-Cr合金在CO2气氛中发生碳化的机理,总结了富CO2气氛中的H2O(g)、SO2、环境温度和合金元素对Ni-Cr合金抗高温腐蚀性能的影响,进而提出未来关于Ni-Cr合金在富CO2气氛中的高温腐蚀需深入研究的问题,包括:解析Ni-Cr合金在不同气氛中热生长Cr2O3膜的微观精细结构,探明CO2、H2O(g)和SO2与稀土元素在氧化膜晶界处的交互作用,关注富CO2气氛中的HCl(g)组分对Ni-Cr合金形成Cr2O3保护膜的影响。

关键词 : Ni-Cr合金,  富CO2气氛,  高温腐蚀    
Abstract:

The thermal power generation industry in China is facing heavy pressure from environmental protection sectors as the “emission peak-carbon neutrality” goal has been proposed. Oxyfuel combustion and operating with high steam parameters are considered promising technologies that can effectively reduce CO2 emissions from coal-fired power plants. However, using these two technologies, the currently used ferritic/martensitic heat-resistant steels and austenitic stainless steels in traditional boilers cannot meet the requirements of good creep strength and corrosion resistance to hot CO2-rich gasses. Thus, nickel-based alloys must be considered. Given that flue gasses related to oxyfuel combustion are characterized by high CO2 concentrations, this work reviews recent research progress on the high-temperature corrosion of Ni-Cr alloys in CO2-rich gasses. Herein, the effect of CO2 on protective Cr2O3 scale formation is introduced, and the related carburization mechanism caused by CO2 ingress is clarified. Moreover, the impacts of H2O(g), SO2, temperature, and alloying elements on the high temperature resistance of Ni-Cr alloys in CO2-rich gasses are summarized. Based on the current findings, future research on high-temperature corrosion of Ni-Cr alloys in CO2-rich gases should focus on the following key points, such as analyzing the microstructure of Cr2O3 scales formed in different gasses; elucidating the interaction of CO2, H2O(g), and SO2 molecules with rare earth elements at grain boundaries of oxide scales; and investigating the effect of HCl(g) impurities in CO2-rich gasses on Cr2O3 scaling of Ni-Cr alloys.

Key words: Ni-Cr alloy    CO2-rich environment    high temperature corrosion
收稿日期: 2023-12-27     
ZTFLH:  TG172.8  
基金资助:国家自然科学基金项目(52301089);江西省重点研发计划项目(20232BBE50007);江西省自然科学基金项目(20224BAB214018)
通讯作者: 谢 云,yun.xie@nchu.edu.cn,主要从事金属材料高温腐蚀的研究;
Corresponding author: XIE Yun, associate professor, Tel: 15827996962, E-mail: yun.xie@nchu.edu.cn
作者简介: 谢 云,男,1988年生,副教授,博士
图1  Ni-30Cr合金在650℃下Ar + 20O2和Ar + 20CO2 (体积分数,%)气氛中腐蚀310 h后的截面SEM像[36,37]
图2  Ni-25Cr和Ni-30Cr合金在700℃下Ar + 20CO2气氛中腐蚀500 h后晶界碳化物的SEM像[37]
图3  Fe-20Cr合金先后在650℃下Ar + 20O2和Ar + 20CO2气氛中腐蚀所形成Cr2O3膜的三维原子探针像[60]
图4  Ni-15Cr合金和纯Ni在650℃下Ar + 20CO2和Ar + 20CO2 + 20H2O气氛中腐蚀后的截面SEM像[42]
图5  Ni-30Cr合金在800℃下Ar + 20CO2 + 20H2O和Ar + 20CO2气氛中腐蚀500 h后的截面SEM像和TEM像[75]
T / oCD˜Cr / (cm2·s-1)NCr(1)NCr(2)
6502.6 × 10-150.31> 0.68
7001.4 × 10-140.280.39
8002.3 × 10-130.240.16
  
图6  Ni-25Cr合金在不同温度下Ar + 20CO2气氛中腐蚀500 h后的截面SEM像[37]
图7  Ni-30Cr-2Ti合金在700℃下Ar + 20CO2 + 20H2O气氛中腐蚀不同时间后的碳化物SEM像[73]
1 Zhang S H, Hu K, Liu X, et al. Corrosion-erosion mechanism and research prospect of bare materials and protective coatings for power generation boiler [J]. Acta Metall. Sin., 2022, 58: 272
doi: 10.11900/0412.1961.2021.00464
1 张世宏, 胡 凯, 刘 侠 等. 发电锅炉材料与防护涂层的磨蚀机制与研究展望 [J]. 金属学报, 2022, 58: 272
doi: 10.11900/0412.1961.2021.00464
2 He H S, Yu L M, Liu C X, et al. Research progress of a novel martensitic heat-resistant steel G115 [J]. Acta Metall. Sin., 2022, 58: 311
doi: 10.11900/0412.1961.2021.00185
2 何焕生, 余黎明, 刘晨曦 等. 新一代马氏体耐热钢G115的研究进展 [J]. 金属学报, 2022, 58: 311.
doi: 10.11900/0412.1961.2021.00185
3 Stanger R, Wall T, Spörl R, et al. Oxyfuel combustion for CO2 capture in power plants [J]. Int. J. Greenhouse Gas Control, 2015, 40: 55
4 Zheng C G, Liu Z H, Xiang J, et al. Fundamental and technical challenges for a compatible design scheme of oxyfuel combustion technology [J]. Engineering, 2015, 1: 139
5 Liu J H. Research and development of oxy-fuel combustion for coal-fired boiler in China [J]. Therm. Power Gener., 2020, 49(7): 48
5 刘建华. 国内燃煤锅炉富氧燃烧技术进展 [J]. 热力发电, 2020, 49(7): 48
6 Bordenet B. Influence of novel cycle concepts on the high-temperature corrosion of power plants [J]. Mater. Corros., 2008, 59: 361
7 Buhre B J P, Elliott L K, Sheng C D, et al. Oxy-fuel combustion technology for coal-fired power generation [J]. Prog. Energy Combust. Sci., 2005, 31: 283
8 Syed A U, Simms N J, Oakey J E. Fireside corrosion of superheaters: Effects of air and oxy-firing of coal and biomass [J]. Fuel, 2012, 101: 62
9 Zeng Z, Natesan K, Cai Z, et al. Effect of coal ash on the performance of alloys in simulated oxy-fuel environments [J]. Fuel, 2014, 117: 133
10 Syed A U, Hussain T, Simms N J, et al. Microscopy of fireside corrosion on superheater materials for oxy-fired pulverised fuel power plants [J]. Mater. High Temp., 2012, 29: 219
11 Stein-Brzozowska G, Maier J, Scheffknecht G. Impact of the oxy-fuel combustion on the corrosion behavior of advanced austenitic superheater materials [J]. Energy Procedia, 2011, 4: 2035
12 Holcomb G R, Tylczak J, Meier G H, et al. Fireside corrosion in oxy-fuel combustion of coal [J]. Oxid. Met., 2013, 80: 599
13 Abellán J P, Olszewski T, Meier G H, et al. The oxidation behaviour of the 9% Cr steel P92 in CO2- and H2O-rich gases relevant to oxyfuel environments [J]. Int. J. Mater. Res., 2010, 101: 287
14 Huczkowski P, Najima S, Chyrkin A, et al. Corrosion behavior of austenitic stainless steels in oxidizing and reducing gases relevant to oxyfuel power plants [J]. JOM, 2018, 70: 1502
15 Zheng Y, Shirani Bidabadi M H, Yang L, et al. Pre-oxidation effect on oxidation behavior of F91 in carbon dioxide at 550oC [J]. Oxid. Met., 2018, 90: 317
16 Xi X T, Kong C, Zhang J Q. Effect of cyclic reaction on corrosion behavior of chromium-containing alloys in CO2 gas at 650oC [J]. Oxid. Met., 2020, 93: 131
17 Cao C, Jiang C Y, Lu J T, et al. Corrosion behavior of austenitic stainless steel with different Cr contents in 700oC coal ash/high sulfur flue-gas environment [J]. Acta Metall. Sin., 2022, 58: 67
17 曹 超, 蒋成洋, 鲁金涛 等. 不同Cr含量的奥氏体不锈钢在700℃煤灰/高硫烟气环境中的腐蚀行为 [J]. 金属学报, 2022, 58: 67
18 Liu Z D, Chen Z Z, He X K, et al. Systematical innovation of heat resistant materials used for 630-700oC advanced ultra-supercritical (A-USC) fossil fired boilers [J]. Acta Metall. Sin., 2020, 56: 539
18 刘正东, 陈正宗, 何西扣 等. 630~700℃超超临界燃煤电站耐热管及其制造技术进展 [J]. 金属学报, 2020, 56: 539
doi: 10.11900/0412.1961.2019.00419
19 Schütze M, Quadakkers W J. Future directions in the field of high-temperature corrosion research [J]. Oxid. Met., 2017, 87: 681
20 Zhao S Q, Xie X S, Smith G D. Corrosion of a new nickel base superalloy in coal-fired boiler environments [J]. Acta Metall. Sin., 2004, 40: 659
20 赵双群, 谢锡善, Smith G D. 新型镍基高温合金在模拟燃煤锅炉环境中的腐蚀 [J]. 金属学报, 2004, 40: 659
21 Mao J X. Latest development of high-temperature metallic materials in 700oC ultra-supercritical units [J]. Electr. Power Constr., 2013, 34(8): 69
21 毛健雄. 700℃超超临界机组高温材料研发的最新进展 [J]. 电力建设, 2013, 34(8): 69
doi: 10.3969/j.issn.1000-7229.2013.08. 013
22 Sun F, Gu Y F, Yan J B, et al. Phenomenological and microstructural analysis of intermediate temperatures creep in a Ni-Fe-based alloy for advanced ultra-supercritical fossil power plants [J]. Acta Mater., 2016, 102: 70
23 Xu Y X, Lu J T, Li W Y, et al. Effect and role of alloyed yttrium on the fireside corrosion behaviour of Ni-Fe based alloys for 750oC ultra-supercritical boiler applications [J]. Corros. Sci., 2018, 143: 148
24 Birks N, Meier G H, Pettit F S. Introduction to the High Temperature Oxidation of Metals [M]. 2nd Ed., Cambridge: Cambridge University Press, 2006: 115
25 Young D J, Zhang J Q. Alloy corrosion by hot CO2 gases [J]. JOM, 2018, 70: 1493
26 Rouillard F, Furukawa T. Corrosion of 9-12Cr ferritic-martensitic steels in high-temperature CO2 [J]. Corros. Sci., 2016, 105: 120
27 Huenert D, Kranzmann A. Impact of oxyfuel atmospheres H2O/CO2/O2 and H2O/CO2 on the oxidation of ferritic-martensitic and austenitic steels [J]. Corros. Sci., 2011, 53: 2306
28 Meier G H, Jung K, Mu N, et al. Effect of alloy composition and exposure conditions on the selective oxidation behavior of ferritic Fe-Cr and Fe-Cr-X alloys [J]. Oxid. Met., 2010, 74: 319
29 Nguyen T D, Zhang J Q, Young D J. Growth of Cr2O3 blades during alloy scaling in wet CO2 gas [J]. Corros. Sci., 2018, 133: 432
30 Nguyen T D, La Fontaine A, Cairney J M, et al. Effects of Si, Mn, and water vapour on the microstructure of protective scales grown on Fe-20Cr in CO2 gas [J]. Mater. High Temp., 2018, 35: 22
31 Yu C, Nguyen T D, Zhang J Q, et al. Sulfur effect on corrosion behavior of Fe-20Cr-(Mn, Si) and Fe-20Ni-20Cr-(Mn, Si) in CO2-H2O at 650oC [J]. J. Electrochem. Soc., 2016, 163: C106
32 Oleksak R P, Tylczak J H, Teeter L, et al. High-temperature corrosion of chromia-forming Ni-based alloys in CO2 containing impurities [J]. High Temp. Corros. Mater., 2023, 100: 597
33 Oleksak R P, Tylczak J H, Holcomb G R, et al. High temperature oxidation of Ni alloys in CO2 containing impurities [J]. Corros. Sci., 2019, 157: 20
34 Zeng Z, Natesan K, Cai Z, et al. Effects of calcium in ash on the corrosion performance of Ni-based alloys in simulated oxy-fuel environment [J]. Fuel, 2016, 178: 10
35 Pan P Y, Li T Y, Wang Y Z, et al. Effect of temperature on hot corrosion of nickel-based alloys for 700oC A-USC power plants [J]. Corros. Sci., 2022, 203: 110350
36 Jiang C Y, Xie Y, Kong C, et al. Corrosion behaviour of Ni-Cr alloys in mixed oxidising gases at 650oC [J]. Corros. Sci., 2020, 174: 108801
37 Xie Y, Zhang J Q, Young D J. Temperature effect on oxidation behavior of Ni-Cr alloys in CO2 gas atmosphere [J]. J. Electrochem. Soc., 2017, 164: C285
38 Nguyen T D, Xie Y, Ding S J, et al. Oxidation behavior of Ni-Cr alloys in CO2 at 700oC [J]. Oxid. Met., 2017, 87: 605
39 Wagner C. Reaktionstypen bei der oxydation von legierungen [J]. Z. Elektrochem., 1959, 63: 772
40 Rapp R A. The transition from internal to external oxidation and the formation of interruption bands in silver-indium alloys [J]. Acta Metall., 1961, 9: 730
41 Wagner C. Theoretical analysis of the diffusion processes determining the oxidation rate of alloys [J]. J. Electrochem. Soc., 1952, 99: 369
42 Xie Y, Zhang J Q, Young D J. Water vapour effects on corrosion of Ni-Cr alloys in CO2 gas at 650oC [J]. Corros. Sci., 2018, 136: 311
43 Wagner C. The theory of the warm-up process [J]. Z. Phys. Chem., 1933, 21: 25
44 Nguyen T D, Zhang J Q, Young D J. Microstructures of chromia scales grown in CO2 [J]. Mater. High Temp., 2015, 32: 16
45 Young D J, Nguyen T D, Felfer P, et al. Penetration of protective chromia scales by carbon [J]. Scr. Mater., 2014, 77: 29
46 Zhu D D, Chen J M, Chen J Z, et al. Atomic origin of CO2-promoted oxidation dynamics of chromia-forming alloys [J]. Acta Mater., 2024, 264: 119578
47 Young D J. High Temperature Oxidation and Corrosion of Metals [M]. 2nd Ed., Amsterdam: Elsevier, 2016: 435
48 Li T F. High Temperature Oxidation and Thermal Corrosion of Metals [M]. Beijing: Chemical Industry Press, 2003: 252
48 李铁藩. 金属高温氧化和热腐蚀 [M]. 北京: 化学工业出版社, 2003: 252
49 Nguyen T D, Zhang J Q, Young D J. Effects of Si, Al and Ti on corrosion of Ni-20Cr and Ni-30Cr alloys in Ar-20CO2 at 700oC [J]. Corros. Sci., 2018, 130: 161
50 Pirón Abellán J, Olszewski T, Penkalla H J, et al. Scale formation mechanisms of martensitic steels in high CO2/H2O-containing gases simulating oxyfuel environments [J]. Mater. High Temp., 2009, 26: 63
51 Nguyen T D, Zhang J Q, Young D J. Martensite formation in Fe-9Cr alloys exposed to low carbon activity gas [J]. Scr. Mater., 2013, 69: 9
52 Gheno T, Monceau D, Zhang J Q, et al. Carburisation of ferritic Fe-Cr alloys by low carbon activity gases [J]. Corros. Sci., 2011, 53: 2767
53 Subramanian G O, Lee H J, Kim S H, et al. Corrosion and carburization behaviour of Ni-xCr binary alloys in a high-temperature supercritical-carbon dioxide environment [J]. Oxid. Met., 2018, 89: 683
54 Lee H J, Kim H, Kim S H, et al. Corrosion and carburization behav-ior of chromia-forming heat resistant alloys in a high-temperature supercritical-carbon dioxide environment [J]. Corros. Sci., 2015, 99: 227
55 Wolf I, Grabke H J. A study on the solubility and distribution of carbon in oxides [J]. Solid State Commun., 1985, 54: 5
56 Wolf I, Grabke H J, Schmidt P. Carbon transport through oxide scales on Fe-Cr alloys [J]. Oxid. Met., 1988, 29: 289
57 Chandra K, Kranzmann A, Saliwan Neumann R, et al. High temperature oxidation behavior of 9-12%Cr ferritic/martensitic steels in a simulated dry oxyfuel environment [J]. Oxid. Met., 2015, 83: 291
58 Otsuka N. Carburization of 9%Cr steels in a simulated oxyfuel corrosion environment [J]. Oxid. Met., 2013, 80: 565
59 Shen J, Liu S, Guo X H, et al. Simultaneous oxidation and carburization of a Fe-9Cr alloy under different oxygen pressures at 800oC [J]. Corros. Sci., 2017, 129: 1
60 Nguyen T D, La Fontaine A, Yang L M, et al. Atom probe study of impurity segregation at grain boundaries in chromia scales grown in CO2 gas [J]. Corros. Sci., 2018, 132: 125
61 Becker P, Young D J. Carburization resistance of nickel-base, heat-resisting alloys [J]. Oxid. Met., 2007, 67: 267
62 Ani M H B, Kodama T, Ueda M, et al. The effect of water vapor on high temperature oxidation of Fe-Cr alloys at 1073 K [J]. Mater. Trans., 2009, 50: 2656
63 Essuman E, Meier G H, Żurek J, et al. The effect of water vapor on selective oxidation of Fe-Cr alloys [J]. Oxid. Met., 2008, 69: 143
64 Essuman E, Meier G H, Żurek J, et al. Enhanced internal oxidation as trigger for breakaway oxidation of Fe-Cr alloys in gases containing water vapor [J]. Scr. Mater., 2007, 57: 845
65 Liu L, Yang Z G, Zhang C, et al. Effect of water vapour on the oxidation of Fe-13Cr-5Ni martensitic alloy at 973 K [J]. Corros. Sci., 2012, 60: 90
66 Young D J, Pint B A. Chromium volatilization rates from Cr2O3 scales into flowing gases containing water vapor [J]. Oxid. Met., 2006, 66: 137
67 Young D J. Effects of water vapour on the oxidation of chromia formers [J]. Mater. Sci. Forum, 2008, 595-598: 1189
68 Holcomb G R. Calculation of reactive-evaporation rates of chromia [J]. Oxid. Met., 2008, 69: 163
69 Wright I G, Dooley R B. A review of the oxidation behaviour of structural alloys in steam [J]. Int. Mater. Rev., 2010, 55: 129
70 Essuman E, Meier G H, Zurek J, et al. Protective and non-protective scale formation of NiCr alloys in water vapour containing high- and low-pO2 gases [J]. Corros. Sci., 2008, 50: 1753
71 Mu N, Jung K Y, Yanar N M, et al. Water vapor effects on the oxidation behavior of Fe-Cr and Ni-Cr alloys in atmospheres relevant to oxy-fuel combustion [J]. Oxid. Met., 2012, 78: 221
72 Mu N, Jung K, Yanar N M, et al. The effects of water vapor and hydrogen on the high-temperature oxidation of alloys [J]. Oxid. Met., 2013, 79: 461
73 Nguyen T D, Zhang J Q, Young D J. Effects of Si, Al and Ti on corrosion of Ni-20Cr and Ni-30Cr alloys in Ar-20CO2-20H2O gas at 700oC [J]. Corros. Sci., 2020, 170: 108702
74 Xie Y. Corrosion behaviour of Ni-Cr-(Fe) alloys in dry and wet CO2 at high temperatures [D]. Sydney: The University of New South Wales, 2018
75 Xie Y, Nguyen T D, Zhang J Q, et al. Corrosion behaviour of Ni-Cr alloys in wet CO2 atmosphere at 700 and 800oC [J]. Corros. Sci., 2019, 146: 28
76 Auchi M, Hayashi S, Toyota K, et al. Effect of water vapor on the high-temperature oxidation of pure Ni [J]. Oxid. Met., 2012, 78: 51
77 Hamdani F, Abe H, Ter-Ovanessian B, et al. Effect of chromium content on the oxidation behavior of Ni-Cr model alloys in superheated steam [J]. Metall. Mater. Trans., 2015, 46A: 2285
78 Jiang C Y, Zhang J Q, Young D J. The effect of water vapor on NiO formation by Ni-Cr alloys at 650oC (HTCPM focus issue, FNS-111) [J]. Oxid. Met., 2021, 96: 57
79 Chen J R, Jiang C Y, Zhang J Q. Corrosion behaviors of Ni-Cr alloys in O2, H2O and H2O + O2 gases at 700oC and the effect of temperature [J]. High Temp. Corros. Mater., 2023, 100: 775
80 Anghel C, Hörnlund E, Hultquist G, et al. Gas phase analysis of CO interactions with solid surfaces at high temperatures [J]. Appl. Surf. Sci., 2004, 233: 392
81 Galerie A, Wouters Y, Caillet M. The kinetic behaviour of metals in water vapour at high temperatures: Can general rules be proposed? [J]. Mater. Sci. Forum, 2001, 369-372: 231
82 Zurek J, Young D J, Essuman E, et al. Growth and adherence of chromia based surface scales on Ni-base alloys in high- and low-pO2 gases [J]. Mater. Sci. Eng., 2008, A477: 259
83 Henry S, Mougin J, Wouters Y, et al. Characterization of chromia scales grown on pure chromium in different oxidizing atmospheres [J]. Mater. High Temp., 2000, 17: 231
84 Michalik M, Hänsel M, Zurek J, et al. Effect of water vapour on growth and adherence of chromia scales formed on Cr in high and low pO2-environments at 1000 and 1050oC [J]. Mater. High Temp., 2005, 22: 213
85 Simon D, Gorr B, Hänsel M, et al. Effect of in-situ gas changes on thermally grown chromia scales formed on Ni-25Cr alloy at 1000oC in atmospheres with and without water vapour [J]. Mater. High Temp., 2015, 32: 238
86 Galerie A, Petit J P, Wouters Y, et al. Water vapour effects on the oxidation of chromia-forming alloys [J]. Mater. Sci. Forum, 2011, 696: 200
87 Mrowec S, Przybylski K. Transport properties of sulfide scales and sulfidation of metals and alloys [J]. Oxid. Met., 1985, 23: 107
88 Huczkowski P, Young D J, Olszewski T, et al. Effect of sulphur on the oxidation behaviour of possible construction materials for heat exchangers in oxyfuel plants in the temperature range 550-700oC [J]. Oxid. Met., 2018, 89: 651
89 Huczkowski P, Najima S, Chyrkin A, et al. Corrosion behavior of candidate heat exchanger materials in oxidizing and reducing gases relevant to oxyfuel power plants [J]. Mater. High Temp., 2018, 35: 275
90 Huczkowski P, Chyrkin A, Singheiser L, et al. Corrosion behavior of candidate heat exchanger materials in oxidizing and reducing gases, relevant to oxyfuel combustion [A]. Corrosion 2016 [C]. Vancouver: NACE International, 2016: 7391
91 Pettit F. Hot corrosion of metals and alloys [J]. Oxid. Met., 2011, 76: 1
92 Gheno T, Gleeson B. On the hot corrosion of nickel at 700oC [J]. Oxid. Met., 2015, 84: 567
93 Lutz B S, Holcomb G R, Meier G H. Determination of the initiation and propagation mechanism of fireside corrosion [J]. Oxid. Met., 2015, 84: 353
94 Grégoire B, Montero X, Galetz M C, et al. Mechanisms of hot corrosion of pure nickel at 700oC: Influence of testing conditions [J]. Corros. Sci., 2018, 141: 211
95 Hu S S, Finklea H, Liu X B. A review on molten sulfate salts induced hot corrosion [J]. J. Mater. Sci. Technol., 2021, 90: 243
doi: 10.1016/j.jmst.2021.03.013
96 Meier G H. Invited review paper in commemoration of over 50 years of oxidation of metals: Current aspects of deposit-induced corrosion [J]. Oxid. Met., 2022, 98: 1
97 Castello P, Guttmann V, Farr N, et al. Laboratory-simulated fuel-ash corrosion of superheater tubes in coal-fired ultra-supercritical-boilers [J]. Mater. Corros., 2000, 51: 786
98 Hussain T, Syed A U, Simms N J. Fireside corrosion of superheater materials in coal/biomass co-fired advanced power plants [J]. Oxid. Met., 2013, 80: 529
99 Liu G M, Yang H C, Liang Q, et al. Corrosion behavior of the Ni-Cr-Fe base superalloy GH984G in a synthetic coal ash and flue gas environment [J]. Acta Metall. Sin. (Engl. Lett.), 2017, 30: 863
100 Hari P R, Arivazhagan N, Rao M N, et al. Hot corrosion studies on alloy 617 OCC in the context of its use in advanced ultra-supercritical (A-USC) power plants [J]. Trans. Indian Inst. Met., 2017, 70: 775
101 Stein-Brzozowska G, Flórez D M, Maier J, et al. Nickel-base superalloys for ultra-supercritical coal-fired power plants: Fireside corrosion. Laboratory studies and power plant exposures [J]. Fuel, 2013, 108: 521
102 Sha C H, Yang L M, Cairney J M, et al. Sulphur diffusion through a growing chromia scale and effects of water vapour [J]. Corros. Sci., 2023, 222: 111410
103 Yu C, Zhang J Q, Young D J. Corrosion behaviour of Fe-Cr-(Mn, Si) ferritic alloys in wet and dry CO2-SO2 atmospheres at 650oC [J]. Oxid. Met., 2018, 90: 97
104 Othman N K, Zhang J Q, Young D J. Temperature and water vapour effects on the cyclic oxidation behaviour of Fe-Cr alloys [J]. Corros. Sci., 2010, 52: 2827
105 Sánchez L, Hierro M P, Pérez F J. Effect of chromium content on the oxidation behaviour of ferritic steels for applications in steam atmospheres at high temperatures [J]. Oxid. Met., 2009, 71: 173
106 Xie Y, Du L X, Liang J J, et al. High temperature oxidation behavior of a novel γ′-strengthened CoNi-base superalloy [J]. High Temp. Corros. Mater., 2024, 101: 211
107 Pint B A, Thomson J K. Effect of oxy-firing on corrosion rates at 600-800oC [A]. Corrosion 2013 [C]. Orlando: NACE International, 2013: 2171
108 Pint B A. Simulated fireside corrosion of Ni-base alloys in oxy-fired conditions at 700-800oC [A]. ASME 2014 Symposium on Elevated Temperature Application of Materials for Fossil, Nuclear, and Petrochemical Industries [C]. Seattle: ASME, 2014: 176
109 Hussain T, Syed A U, Simms N J. Trends in fireside corrosion damage to superheaters in air and oxy-firing of coal/biomass [J]. Fuel, 2013, 113: 787
110 Saunders S R J, Monteiro M, Rizzo F. The oxidation behaviour of metals and alloys at high temperatures in atmospheres containing water vapour: A review [J]. Prog. Mater. Sci., 2008, 53: 775
111 Raynaud G M, Rapp R A. In situ observation of whiskers, pyramids and pits during the high-temperature oxidation of metals [J]. Oxid. Met., 1984, 21: 89
112 Larsson K, Björkman H, Hjort K. Role of water and oxygen in wet and dry oxidation of diamond [J]. J. Appl. Phys., 2001, 90: 1026
113 Lu J T, Yang Z, Li Y, et al. Effect of alloying chemistry on fireside corrosion behavior of Ni-Fe-based superalloy for ultra-supercritical boiler applications [J]. Oxid. Met., 2018, 89: 609
114 Xu Y X, Lu J T, Yang X W, et al. Effect and role of alloyed Nb on the air oxidation behaviour of Ni-Cr-Fe alloys at 1000oC [J]. Corros. Sci., 2017, 127: 10
115 Xie Y, Zhang J Q, Young D J, et al. Effect of Fe on corrosion of Ni-20Cr and Ni-30Cr alloys in wet CO2 gas at 650 and 700oC [J]. Corros. Sci., 2019, 154: 129
116 Xie Y, Liang T, Zhang J Q, et al. Effects of Fe on oxidation of Ni-20Cr and Ni-30Cr alloys at 800oC in dry CO2 gas [J]. Corros. Sci., 2020, 173: 108777
117 Xie Y, Zhang J Q, Young D J. Effects of Fe on oxidation of Ni-20Cr and Ni-30Cr alloys at 800oC in wet CO2 gas [J]. Oxid. Met., 2020, 94: 219
118 Million B, Růžičková J, Vřešťál J. Diffusion in Fe-Ni-Cr alloys with an F.C.C. lattice [J]. Mater. Sci. Eng., 1985, 72: 85
119 Duh J G, Dayananda M A. Interdiffusion in Fe-Ni-Cr alloys at 1100oC [J]. Defect Diffus. Forum, 1991, 39: 1
120 Xu Y X, Lu J T, Huang J Y, et al. Impact of iron and chromium on coal ash corrosion behavior of Ni-Cr-Co based alloy for advanced ultra-supercritical power plants [J]. Corrosion, 2018, 74: 1446
121 Colwell J A, Rapp R A. Reactions of Fe-Cr and Ni-Cr alloys in CO/CO2 gases at 850 and 950oC [J]. Metall. Trans., 1986, 17A: 1065
[1] 曹超, 蒋成洋, 鲁金涛, 陈明辉, 耿树江, 王福会. 不同Cr含量的奥氏体不锈钢在700℃煤灰/高硫烟气环境中的腐蚀行为[J]. 金属学报, 2022, 58(1): 67-74.
[2] 包飞洋, 李艳芬, 王光全, 张家榕, 严伟, 石全强, 单以银, 杨柯, 许斌, 宋丹戎, 严明宇, 魏学栋. ODS钢在600和700 ℃静态Pb-Bi共晶中的腐蚀行为及机理[J]. 金属学报, 2020, 56(10): 1366-1376.
[3] 郭策安, 陈明辉, 廖依敏, 苏北, 谢冬柏, 朱圣龙, 王福会. 模拟燃气热冲击条件下搪瓷基复合涂层的防护机理研究[J]. 金属学报, 2018, 54(12): 1825-1832.
[4] 彭晓, 王福会. 纳米晶金属材料的高温腐蚀行为*[J]. 金属学报, 2014, 50(2): 202-211.
[5] 杨军 贺志荣 王芳 王永善. Cr掺杂对Ti-Ni形状记忆合金相变和循环形变特性的影响[J]. 金属学报, 2011, 47(2): 157-162.
[6] 李秀艳; 戎利建; 李依依 . 晶界η相对Fe-Ni-Cr奥氏体合金力学性能的影响[J]. 金属学报, 2005, 41(11): 1155-1158 .
[7] 张轲; 牛焱; 吴维tao . 2.25CrMo 钢在还原性含氯气氛中的高温腐蚀行为[J]. 金属学报, 2003, 39(5): 541-543 .
[8] 牛焱; 李远士 . 在交替氧化—硫化气氛中12Cr钢的高温腐蚀[J]. 金属学报, 2000, 36(8): 851-853 .
[9] 曹中秋; 牛焱 . Cu-Cr-Ni合金在800℃, 0.1 MPa纯氧气中的氧化[J]. 金属学报, 2000, 36(6): 647-650 .