| 溶质Ti对Al-Ti-B中间合金细化Al影响的新认识:TiB2粒子的动力学行为及溶质Ti的影响 |
张丽丽1, 江鸿翔1, 赵九洲1( ), 李璐2, 孙倩1 |
1 中国科学院金属研究所 沈阳 110016 2 国家知识产权局专利局专利审查协作天津中心 天津 300304 |
|
| A New Understanding Toward Effect of Solute Ti on Grain Refinement of Aluminum by Al-Ti-B Master Alloy: Kinetic Behaviors of TiB2 Particles and Effect of Solute Ti |
Lili ZHANG1, Hongxiang JIANG1, Jiuzhou ZHAO1( ), Lu LI2, Qian SUN1 |
1 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2 Patent Examination Cooperation Tianjin Center of the Patent Office. SIPO., Tianjin 300304, China |
引用本文:
张丽丽, 江鸿翔, 赵九洲, 李璐, 孙倩. 溶质Ti对Al-Ti-B中间合金细化Al影响的新认识:TiB2粒子的动力学行为及溶质Ti的影响[J]. 金属学报, 2017, 53(9): 1091-1100.
Lili ZHANG,
Hongxiang JIANG,
Jiuzhou ZHAO,
Lu LI,
Qian SUN.
A New Understanding Toward Effect of Solute Ti on Grain Refinement of Aluminum by Al-Ti-B Master Alloy: Kinetic Behaviors of TiB2 Particles and Effect of Solute Ti[J]. Acta Metall Sin, 2017, 53(9): 1091-1100.
| [1] | Quested T E.Understanding mechanisms of grain refinement of aluminium alloys by inoculation[J]. Mater. Sci. Technol., 2004, 20: 1357 | | [2] | Wannasin J, Canyook R, Wisutmethangoon S, et al.Grain refinement behavior of an aluminum alloy by inoculation and dynamic nucleation[J]. Acta Mater., 2013, 61: 3897 | | [3] | Wang H X, Zhang G P, Xu C X, et al.Effect of mechanical vibration on grain refinement and solidification shrinkage of aluminum[J]. Res. Stud. Foundry Equip., 2007, (1): 28(王红霞, 张国平, 许春香等. 机械振动对纯Al晶粒细化及凝固收缩的影响[J]. 铸造设备研究, 2007, (1): 28) | | [4] | Yu J B.Influence of superposing electricity and magnetic field on the solidification structure of metals [D]. Shanghai: Shanghai University, 2009(余建波. 电、磁复合效应对金属凝固组织的影响 [D]. 上海: 上海大学, 2009) | | [5] | Zhao Z X.The homogeneity of casting alloy process effected by ultrasonic[J]. Hot Working Technol., 1999, (5): 10(赵忠兴. 超声波对合金结晶过程的均匀化作用[J]. 热加工工艺, 1999, (5): 10) | | [6] | Li J W, Tao Y Z.Effect of ultrasonic on structure of aluminum alloy ingots[J]. Foundry Technol., 2004, 25: 593(李军文, 桃野正. 超声波对铝合金铸锭组织的影响[J]. 铸造技术, 2004, 25: 593) | | [7] | Han Y F, Shu D, Wang J, et al.Microstructure and grain refining performance of Al-5Ti-1B master alloy prepared under high-intensity ultrasound[J]. Mater. Sci. Eng., 2006, A430: 326 | | [8] | Birol Y.Efficiency of binary and ternary alloys from Al-Ti-B system in grain refining aluminium foundry alloys[J]. Int. J. Cast Met. Res., 2013, 26: 283 | | [9] | Easton M, StJohn D. Grain refinement of aluminum alloys: Part II. Confirmation of, and a mechanism for, the solute paradigm[J]. Metall. Mater. Trans., 1999, 30A: 1625 | | [10] | Fan Z, Wang Y, Zhang Y, et al.Grain refining mechanism in the Al/Al-Ti-B system[J]. Acta Mater., 2015, 84: 292 | | [11] | Qin T, Fan Z.Reconstruction of 2D Al3Ti on TiB2 in an aluminum melt[J]. Mater. Sci. Eng., 2011, 27: 012004 | | [12] | Maxwell I, Hellawell A.A simple model for grain refinement during solidification[J]. Acta Metall., 1975, 23: 229 | | [13] | Greer A L, Bunn A M, Tronche A, et al.Modelling of inoculation of metallic melts: Application to grain refinement of aluminium by Al-Ti-B[J]. Acta Mater., 2000, 48: 2823 | | [14] | Quested T E, Greer A L.The effect of the size distribution of inoculant particles on as-cast grain size in aluminium alloys[J]. Acta Mater., 2004, 52: 3859 | | [15] | Quested T E, Greer A L.Grain refinement of Al alloys: Mechanisms determining as-cast grain size in directional solidification[J]. Acta Mater., 2005, 53: 4643 | | [16] | Easton M A, StJohn D H. A model of grain refinement incorporating alloy constitution and potency of heterogeneous nucleant particles[J]. Acta Mater., 2001, 49: 1867 | | [17] | Easton M A, StJohn D H. An analysis of the relationship between grain size, solute content, and the potency and number density of nucleant particles[J]. Metall. Mater. Trans., 2005, 36A: 1911 | | [18] | Easton M A, StJohn D H. Improved prediction of the grain size of aluminum alloys that includes the effect of cooling rate[J]. Mater. Sci. Eng., 2008, A486: 8 | | [19] | Jones G P, Pearson J.Factors affecting the grain-refinement of aluminum using titanium and boron additives[J]. Metall. Trans., 1976, 7B: 223 | | [20] | He J, Zhao J Z, Ratke L.Solidification microstructure and dynamics of metastable phase transformation in undercooled liquid Cu-Fe alloys[J]. Acta Mater., 2006, 54: 1749 | | [21] | Zhao J Z, Li H L, Zhang X F, et al.Microstructure evolution during a liquid-liquid decomposition under the common action of the nucleation, growth and Ostwald ripening of droplets[J]. Int. J. Mater. Res., 2009, 100: 46 | | [22] | Takaimchi I, Roderick I L, translated by Xian A P, Wang L W. The Physical Properties of Liquid Metals [M]. Beijing: Science Press, 2006: 73(Takaimchi I, Roderick I L著, 冼爱平, 王连文译. 液态金属的物理性能 [M]. 北京: 科学出版社, 2006: 73) | | [23] | Sun X Y.Study on refinement mechanism of Al-Ti-B and Al-Ti-C master alloys in aluminum and its alloys [D]. Beijing: Tsinghua University, 2011(孙雪迎. Al-Ti-B、Al-Ti-C中间合金细化铝及铝合金机制研究 [D]. 北京: 清华大学, 2011) | | [24] | Sigworth G K.The grain refining of aluminum and phase relationships in the Al-Ti-B system[J]. Metall. Trans., 1984, 15A: 277 | | [25] | Zhao J Z, Gao L L, He J, et al.Liquid-liquid phase transformation kinetics of an atomized Al-Pb alloy drop[J]. Acta Metall. Sin., 2006, 42: 113(赵九洲, 高玲玲, 何杰等. Al-Pb合金雾化液滴的液-液相变动力学[J]. 金属学报, 2006, 42: 113) | | [26] | Liu D M, Zhao J Z, Ye H Q.Modeling of the solidification of gas-atomized alloy droplets during spray forming[J]. Acta Metall. Sin., 2003, 39: 375(刘东明, 赵九洲, 叶恒强. 喷射成形中金属液滴凝固过程的计算机模拟[J]. 金属学报, 2003, 39: 375) | | [27] | Teng X R.Surfactant Chemistry [M]. Beijing: Chemical Industry Press, 2009: 46(滕新荣. 表面物理化学 [M]. 北京: 化学工业出版社, 2009: 46) | | [28] | Kaptay G.Partial surface tension of components of a solution[J]. Langmuir, 2015, 31: 5796 | | [29] | Kaptay G.Modelling equilibrium grain boundary segregation, grain boundary energy and grain boundary segregation transition by the extended Butler equation[J]. J. Mater. Sci., 2016, 51: 1738 | | [30] | Men H, Fan Z Y.An analytical model for solute segregation at liquid metal/solid substrate interface[J]. Metall. Mater. Trans., 2014, 45A: 5508 | | [31] | Han Y F.Study on Al-5Ti-1B master alloy prepared under ultrasound and α-Al/diboride interface [D]. Shanghai: Shanghai Jiao Tong University, 2007(韩延峰. 超声制备Al-5Ti-1B中间合金及α-Al/异质核心界面研究 [D]. 上海: 上海交通大学, 2007) | | [32] | Feuerbacher B, Hamacher H, Naumann R J.Materials Sciences in Space: A Contribution to the Scientific Basis of Space Processing[M]. Berlin: Springer-Verlag, 1986: 11 |
|
|