| Al-Si-Ge钎料钎焊Cu/Al接头组织与性能研究 |
牛志伟,叶政,刘凯凯,黄继华( ),陈树海,赵兴科 |
| 北京科技大学材料科学与工程学院 北京 100083 |
|
| Microstructure and Property of Cu/Al Joint Brazed with Al-Si-Ge Filler Metal |
Zhiwei NIU,Zheng YE,Kaikai LIU,Jihua HUANG( ),Shuhai CHEN,Xingke ZHAO |
| School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China |
引用本文:
牛志伟,叶政,刘凯凯,黄继华,陈树海,赵兴科. Al-Si-Ge钎料钎焊Cu/Al接头组织与性能研究[J]. 金属学报, 2017, 53(6): 719-725.
Zhiwei NIU,
Zheng YE,
Kaikai LIU,
Jihua HUANG,
Shuhai CHEN,
Xingke ZHAO.
Microstructure and Property of Cu/Al Joint Brazed with Al-Si-Ge Filler Metal[J]. Acta Metall Sin, 2017, 53(6): 719-725.
| [1] | Ning F Z.Low temperature friction welding of aluminum to copper[J]. Acta Metall. Sin., 1978, 14: 179 | | [1] | (宁斐章. 铝-铜低温摩擦焊[J]. 金属学报, 1978, 14: 179) | | [2] | Zhang H T, Liu D, Feng J C, et al.Reactive contact brazing between Aluminium alloy and copper by high frequency induction metho[J]. Trans. China Weld. Inst., 2012, 33(3): 89 | | [2] | (张洪涛, 刘多, 冯吉才等. 铝/铜高频感应接触反应钎焊[J]. 焊接学报, 2012, 33(3): 89) | | [3] | Cong Q, Xu F M, Tan Y, et al.Influence of heat treatment on microstructure and mechanical properties of Al/Al-Cu graded materials[J]. Acta Metall. Sin.(Engl. Lett.), 2011, 24: 118 | | [4] | Easton D, Zhang Y X, Wood J, et al. Brazing development and interfacial metallurgy study of tungsten and copper joints with eutectic gold copper brazing alloy [J]. Fusion Eng. Des., 2015, 98-99: 1956 | | [5] | Fu W, Song X G, Hu S P, et al.Brazing copper and alumina metallized with Ti-containing Sn0.3Ag0.7Cu metal powder[J]. Mater. Des., 2015, 87: 579 | | [6] | Xing F, Yao J, Liang J W, et al.Influence of intermetallic growth on the mechanical properties of Zn-Sn-Cu-Bi/Cu solder joints[J]. J. Alloys Compd., 2015, 649: 1053 | | [7] | Zhou J, Sun Y S, Xue F.Microstructures and properties of Sn-Zn-Bi solder alloys[J]. Acta Metall. Sin., 2005, 41: 743 | | [7] | (周健, 孙扬善, 薛烽. 低熔点Sn-Zn-Bi无铅钎料的组织和性能[J]. 金属学报, 2005, 41: 743) | | [8] | Huang M L, Kang N, Zhou Q, et al.Effect of Ni content on mechanical properties and corrosion behavior of Al/Sn-9Zn-xNi/Cu Joints[J]. J. Mater. Sci. Technol., 2012, 28: 844 | | [9] | Xiao Y, Ji H J, Li M Y, et al.Ultrasound-assisted brazing of Cu/Al dissimilar metals using a Zn-3Al filler metal[J]. Mater. Des., 2013, 52: 740 | | [10] | Ji F, Xue S B, Lou J Y, et al.Microstructure and properties of Cu/Al joints brazed with Zn-Al filler metals[J]. Trans. Nonferrous. Met. Soc. China, 2012, 22: 281 | | [11] | Ji F, Xue S B.Growth behaviors of intermetallic compound layers in Cu/Al joints brazed with Zn-22Al and Zn-22Al-0.05Ce filler metals[J]. Mater. Des., 2013, 51: 907 | | [12] | Yan F, Xu D R, Wu S C, et al.Microstructure and phase constitution near the interface of Cu/3003 torch brazing using Al-Si-La-Sr filler[J]. J. Mech. Sci. Technol., 2012, 26: 4089 | | [13] | Xia C Z, Li Y J, Puchkov U A, et al.Microstructure and phase constitution near the interface of Cu/Al vacuum brazing using Al-Si filler metal[J]. Vacuum, 2008, 82: 799 | | [14] | Yang H, Huang J H, Chen S H, et al.Influence of the composition of Zn-Al filler metal on the interfacial structure and property of Cu/Zn-Al/Al brazed joint[J]. Acta Metall. Sin., 2015, 51: 364 | | [14] | (羊浩, 黄继华, 陈树海等. Zn-Al钎料成分对Cu/Zn-Al/Al钎焊接头界面结构及性能的影响[J]. 金属学报, 2015, 51: 364) | | [15] | Zhang Q Y, Zhuang H S.Brazing and Soldering Manual [M]. Beijing: China Machine Press, 2008: 55 | | [15] | (张启运, 庄鸿寿. 钎焊手册 [M]. 北京: 机械工业出版社, 2008: 55) | | [16] | Zuo K, Zuo T J, Qiu G C, et al.Comparison of corrosion resistance between Al-Si brazing filler and Al-Zn brazing filler [A]. Proceedings of the Eleventh National Symposium on Refrigerators, Air Conditioners and Compressors[C]. Chuzhou: Chinese Association of Refrigeration, 2012: 293 | | [16] | (左柯, 左铁军, 邱国才等. Al-Si钎料和Al-Zn钎料抗腐蚀性能比较 [A]. 第十一届全国电冰箱(柜)、空调器及压缩机学术交流大会论文集[C]. 滁州: 中国制冷学会, 2012: 293) | | [17] | Zheng J F, Chen D J, Cai Q, et al.Comparison of corrosion resis tance between Al-Si brazing filler and Al-Zn brazing filler[J]. Household Appl. Technol., 2013, (10): 78 | | [17] | (郑建峰, 陈德娟, 蔡蔷等. Al-Si钎料和Al-Zn钎料耐蚀性能对比研究[J]. 家电科技, 2013, (10): 78) | | [18] | Hosch T, Napolitano R E.The effect of the flake to fiber transition in silicon morphology on the tensile properties of Al-Si eutectic alloys[J]. Mater. Sci. Eng., 2010, A528: 226 | | [19] | Luo W, Wang L T, Wang Q M, et al.A new filler metal with low contents of Cu for high strength aluminum alloy brazed joints[J]. Mater. Des., 2014, 63: 263 | | [20] | Liu H J, Shen J J.Progress in welding process of Al/Cu dissimilar metals[J]. Weld. Join., 2009, (3): 14 | | [20] | (刘会杰, 沈俊军. 铝/铜异种材料的焊接研究[J]. 焊接, 2009, (3): 14) | | [21] | Niu Z W, Huang J H, Chen S H, et al.Effects of germanium additions on microstructures and properties of Al-Si filler metals for brazing aluminum[J]. Trans. Nonferrous. Met. Soc. China, 2016, 26: 775 | | [22] | Schubert T H, Loser W, Teresiak A, et al.Preparation and phase transformations of melt-spun Al-Ge-Si brazing foils[J]. J. Mater. Sci., 1997, 32: 2181 | | [23] | Niu Z W, Huang J H, Yang H, et al.Preparation and properties of a novel Al-Si-Ge-Zn filler metal for brazing aluminum[J]. J. Mater. Eng. Perform., 2015, 24: 2327 | | [24] | Yang L S, Wang H M, Chen Q D.High Aluminum Zn Alloys [M]. Xi'an: Northwestern Polytechnic University Press, 1997: 17 | | [24] | (杨留栓, 王洪敏, 陈全德. 高铝锌合金 [M]. 西安: 西北工业大学出版社, 1997: 17) | | [25] | Zhang M, Xue S B, Dai W, et al.Effect of Ag on properties of Zn-Al brazing filler metal[J]. Trans. China Weld. Inst., 2010, 31(10): 73 | | [25] | (张满, 薛松柏, 戴玮等. Ag元素对Zn-Al钎料性能的影响[J]. 焊接学报, 2010, 31(10): 73) |
|
|