| 晶粒及晶界特征对高锰奥氏体TWIP钢抗腐蚀能力的影响* |
袁晓云,陈礼清( ) |
| 东北大学轧制技术及连轧自动化国家重点实验室, 沈阳 110819 |
|
| EFFECT OF GRAIN AND GRAIN BOUNDARY FEATURESON ANTI-CORROSION ABILITY OF A HIGH MANGANESE AUSTENITIC TWIP STEEL |
Xiaoyun YUAN,Liqing CHEN( ) |
| State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819, China |
引用本文:
袁晓云, 陈礼清. 晶粒及晶界特征对高锰奥氏体TWIP钢抗腐蚀能力的影响*[J]. 金属学报, 2016, 52(10): 1345-1352.
Xiaoyun YUAN,
Liqing CHEN.
EFFECT OF GRAIN AND GRAIN BOUNDARY FEATURESON ANTI-CORROSION ABILITY OF A HIGH MANGANESE AUSTENITIC TWIP STEEL[J]. Acta Metall Sin, 2016, 52(10): 1345-1352.
| [1] | Shu X L, Yan N H, Shu R Y, Peng Y Z.Corros Sci, 2013; 66: 211 | | [2] | Gollapudi S.Corros Sci, 2012; 62: 90 | | [3] | Qian X R, Chou Y T.Phil Mag, 1982; 45A: 1075 | | [4] | Erb U, Gleiter H, Schwitzgebel G.Acta Metall, 1982; 30: 1377 | | [5] | Bennett B W, Pickering H W.Metall Trans, 1987; 18A: 1117 | | [6] | Watanabe T.Res Mech, 1984; 11: 47 | | [7] | Randle V.Acta Mater, 2004; 52: 4067 | | [8] | Watanabe T.Mater Sci, 2011; 46: 4095 | | [9] | Lin P, Palumbo G, Erb U.Scr Metall Mater, 1995; 33: 1387 | | [10] | Lin P, Palumbo G, Aust K T.Scr Mater, 1997; 36: 1145 | | [11] | Lehockey E M, Limoges D, Palumbo G, Sklarchuk J, Tomantschger K, Vincze A.J Power Sources, 1999; 78: 79 | | [12] | Xia S, Zhou B X, Chen W J, Wang W G.Scr Mater, 2006; 54: 2019 | | [13] | Palumbo G, Aust K T.Acta Metall Mater, 1990; 38: 2343 | | [14] | Cheung C, Erb U, Palumbo G.Mater Sci Eng, 1994; A185: 39 | | [15] | Alexandreanu B, Was G S.Scr Mater, 2006; 54: 1047 | | [16] | Shimada M, Kokawa H, Wang Z J, Sato Y S.Acta Mater, 2002; 50: 2331 | | [17] | West E A, Was G S.Nucl Mater, 2009; 392: 264 | | [18] | Michiuchi M, Kokawa H, Wang Z J, Sato Y S, Sakai K.Acta Mater, 2006; 54: 5179 | | [19] | Kobayashi S, Kobayashi R, Watanabe T.Acta Mater, 2016; 102: 397 | | [20] | Emregul K, Atakol O.Mater Chem Phys, 2004; 83: 373 | | [21] | Ju H, Kai Z P, Li Y.Corros Sci, 2008; 50: 865 | | [22] | Luo J, Zhang Y, Zhong Q D, Zhang L, Zhu Z Y.Corros Prot, 2014; 33: 349 | | [22] | (罗检, 张勇, 钟庆东, 张磊, 朱振宇, 腐蚀与防护, 2014; 33: 349) | | [23] | Wang F C, Dong Y, Han X, Sun Z X, Qi Y H.Light Alloy Fabr Technol, 2013; 41(6): 33 | | [23] | (王凤春, 董影, 韩啸, 孙兆霞, 祁艳华. 轻合金加工技术, 2013; 41(6): 33) | | [24] | Randle V.Acta Mater, 1999; 47: 4186 | | [25] | Schuh C A, Kumar M, KingW E.Acta Mater, 2003; 51: 68. | | [26] | Watanabe T.Res Mech, 1984; 11: 47. | | [27] | Watanabe T.Scr Metall Mater, 1992; 27: 1497 | | [28] | Randle V.Acta Mater, 2004; 52: 4067 |
|
|