Please wait a minute...
金属学报  2013, Vol. 49 Issue (11): 1281-1285    DOI: 10.3724/SP.J.1037.2013.00536
  综述 本期目录 | 过刊浏览 |
TiAl基金属间化合物熔模精密铸造研究进展
陈玉勇1,2),贾燚1,2),肖树龙1,2),田竟2),徐丽娟2)
1) 哈尔滨工业大学金属精密热加工国家级重点实验室, 哈尔滨 150001
2) 哈尔滨工业大学材料科学与工程学院, 哈尔滨 150001
REVIEW OF THE INVESTMENT CASTING OF TiAl-BASED INTERMETALLIC ALLOYS
CHEN Yuyong1,2), JIA Yi1,2), XIAO Shulong1,2), TIAN Jing 2), XU Lijuan 2)
1) National Key Laboratory of Science and Technology on Precision Heat Processing of Metals, Harbin Institute of Technology, Harbin 150001
2) School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001
引用本文:

陈玉勇,贾燚,肖树龙,田竟,徐丽娟. TiAl基金属间化合物熔模精密铸造研究进展[J]. 金属学报, 2013, 49(11): 1281-1285.
CHEN Yuyong, JIA Yi, XIAO Shulong, TIAN Jing, XU Lijuan. REVIEW OF THE INVESTMENT CASTING OF TiAl-BASED INTERMETALLIC ALLOYS[J]. Acta Metall Sin, 2013, 49(11): 1281-1285.

全文: PDF(797 KB)  
摘要: 

TiAl基金属间化合物作为一种新型轻质高温结构材料,在航空航天和汽车等领域具有广阔的应用前景.熔模精密铸造是目前制备TiAl基金属间化合物构件的主要方法之一.本文主要介绍了TiAl基金属间化合物的合金设计、熔模精密铸造技术及应用研究概况,并对TiAl基金属间化合物熔模精密铸造技术发展提出了展望.

关键词 : TiAl 基金属间化合物,  熔模精密铸造,  陶瓷型壳,  应用研究    
Abstract:

TiAl-based intermetallic alloys are emerging as a new generation light—weight, high temperature structural materials and possess wide capacities of engineering applications in aeronautics, space and automobile industries. Near—net—shape casting is a commonly used manufacturing method for TiAl—based alloys. In this paper, the evolution of the alloy design and investment casting technology of TiAl—based alloys are reviewed. The prospects of the investment casting of TiAl—based alloys are also represented.

Key words: TiAl—based intermetallic alloy    investment casting    ceramic shell    application research
收稿日期: 2013-09-02     
基金资助:

国家自然科学基金项目51001040和51371064资助

作者简介: 陈玉勇, 男, 1956年生, 教授

[1] Kim Y W.  JOM, 1995; 47: 39

[2] Carneiro T, Kim Y W.  Intermetallics, 2005; 13: 1000
[3] McQuay P A, Sikka V K. In: Westbrook J H, Fleischer R L, eds.,Intermetallic Compounds. Chichester: John Wiley & Sons Ltd., 2002: 591
[4] Chen G L, Wang J G, Sun Z Q, Ye H Q.  Intermetallics, 1994; 2: 31
[5] Tetsui T, Shindo K, Kobayashi S, Takeyama M.  Scr Mater, 2002; 47: 399
[6] Zhang W J, Liu Z C, Chen G L, Kim Y W.  Mater Sci Eng, 1999; A271: 416
[7] Jung H G, Kim K Y.  Oxid Met, 2002; 58: 197
[8] Wallgram W, Schmolzer T, Cha L M, Das G, Guther V, Clemens H.  Int J Mater Res, 2009;100: 1021
[9] Hu D, Wu X, Loretto M H.  Intermetallics, 2005; 13: 914
[10] Jones S, Yuan C.  J Mater Process Technol, 2003; 135: 258
[11] Su Y Q, Guo J J, Jia J.  J Aeron Mater, 1999; 19(4): 11
(苏彦庆, 郭景杰, 贾均. 航空材料学报, 1999; 19(4): 11)
[12] Kuang J P, Harding R A, Campbell J.  Mater Sci Eng, 2002; A329: 31
[13] Kim M G, Kim Y J.  Met Mater Int, 2002; 8: 289
[14] Nowak R, Lanata T, Sobczak N, Ricci E, Giuranno D, Novakovic R,Holland—Moritz D, Egry I.  J Mater Sci, 2010; 45: 1993
[15] Kuang J P, Harding R A, Campbell J.  Mater Sci Technol, 2000; 16: 1007
[16] Cui R J, Gao M, Zhang H, Gong S K.  J Mater Process Technol, 2010; 210: 1190
[17] Teodoro O, Barbosa J, Naia M D, Moutinho A M C.  Appl Surf Sci, 2004; 231: 854
[18] Tetsui T, Kobayashi T, Mori T, Kishimoto T, Harada H.  Mater Trans, 2010; 51: 1656
[19] Lapin J, Ondrus L, Nazmy M.  Intermetallics, 2002; 10: 1019
[20] Liu A H, Li B S, Nan H, Sui Y W, Yu J, Guo J J, Fu H Z.  Rare Met Mater Eng, 2007; 36:1975
(刘爱辉, 李邦盛, 南海, 隋艳伟, 于杰, 郭景杰, 傅恒志. 稀有金属材料与工程,2007; 36: 1975)
[21] Barbosa J, Puga H, Ribeiro C S, Teodoro O, Monteiro A C.  Int J Cast Met Res, 2006; 19:331
[22] Cheng X, Yuan C, Green N, Withey P.  Metall Mater Trans, 2013; 44A: 888
[23] Larsen D E, Christodoulou L, Kampe S L, Sadler P.  Mater Sci Eng, 1991; A144: 45
[24] Jia Q, Cui Y Y, Yang R.  J Mater Sci, 2006; 41: 3045
[25] Kim M G, Kim S K, Kim Y J.  Mater Trans, 2002; 43: 745
[26] Yuan C, Jones S.  J Eur Ceram Soc, 2003; 23: 399
[27] Chen Y F, Xiao S L, Tian J, Xu L J, Kong F T, Chen Y Y.  China Foundry, 2011; 8: 9
[28] Liu K, Ma Y C, Gao M, Rao G B, Li Y Y, Wei K, Wu X H, Loretto M H.Intermetallics, 2005; 13: 925
[29] Baake E, Nacke B, Bernier F, Vogt M, Muhlbauer A.  Compel, 2003; 22: 88
[30] Mi J, Harding R A, Wickins M, Campbell J.  Intermetallics, 2003; 11: 377
[31] Gomes F, Barbosa J, Ribeiro C S.  Intermetallics, 2008; 16: 1292
[32] Barbosa J, Ribeiro C S, Monteiro A C.  Intermetallics, 2007; 15: 945
[33] Tetsui T, Kobayashi T, Kishimoto A, Harada H.  Intermetallics, 2012; 20: 16
[34] Sung S Y, Kim Y J.  Intermetallics, 2007; 15: 468
[35] Campbell J.  Int J Metalcasting, 2012; 6: 7
[36] Harding R A, Wickins M, Wang H, Djambazov G, Pericleous K A.Intermetallics, 2011; 19: 805
[37] Noda T.  Intermetallics, 1998; 6: 709
[38] Tetsui T.  Mater Sci Eng, 2002; A329: 582
[39] Aguilar J, Schievenbusch A, Kattlitz O.  Intermetallics, 2011; 19: 757
[40] Lavery N P, Jarvis D J, Voss D.  Intermetallics, 2011; 19: 787
[41] Reitz J, Lochbichler C, Friedrich B.  Intermetallics, 2011; 19: 762
[42] Jarvis D J, Voss D.  Mater Sci Eng, 2005; A413: 583
[1] 陈晓燕,金喆,白雪峰,周亦胄,金涛,孙晓峰. C对一种镍基高温合金与陶瓷型壳界面反应及润湿性的影响*[J]. 金属学报, 2015, 51(7): 853-858.