| 制备参量对BaZrO3:Ce纳米粉体形貌和发光性能的影响 |
| 李玉玲1), 马伟民1), 闻雷2), 温强1), 苑晓宇3) |
1) 沈阳化工大学应用化学学院辽宁省稀土化学及应用重点实验室, 沈阳 110142
2) 中国科学院金属研究所沈阳材料科学国家(联合)实验室, 沈阳 110016
3) 沈阳大学机械工程学院, 沈阳 110044 |
|
| INFLUENCES OF PREPARATION PARAMETERS ON MORPHOLOGY AND PHOTOLUMINESCENCE PROPERTY OF BaZrO3:Ce NANO-POWDERS |
| LI Yuling1), MA Weimin1), WEN Lei2), WEN Qiang1), YUAN Xiaoyu3) |
1) Liaoning Province Key Laboratory for Rare-Earth Chemistry and Applying, College of Applied Chemistry, Shenyang University of Chemical Technology, Shenyang 110142
2) Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
3) College of Mechanical Engineering, Shenyang University, Shenyang 110044 |
引用本文:
李玉玲 马伟民 闻雷 温强 苑晓宇. 制备参量对BaZrO3:Ce纳米粉体形貌和发光性能的影响[J]. 金属学报, 2011, 47(1): 95-101.
,
,
,
,
.
INFLUENCES OF PREPARATION PARAMETERS ON MORPHOLOGY AND PHOTOLUMINESCENCE PROPERTY OF BaZrO3:Ce NANO-POWDERS[J]. Acta Metall Sin, 2011, 47(1): 95-101.
| [1] Nikl M, Mares J A, Solovieva N, Li H L, Liu X J, Huang L P, Fontana I, Fasoli M, Vedda A, Ambrosio C D. J Appl Phy, 2007; 101: 33515[2] Serivalsatit K, Kokuoz B, Yazgan–Kokuoz B, Kennedy M, Ballato J. J Am Ceram Soc, 2010; 93: 1320[3] Ramirez M O,Wisdom J, Li H F, Aung Y L, Stitt J, Messing G L, Dierolf V, Liu Z W, Ikesue A, Byer R L, Gopalan V. Optics Express, 2008; 16: 5965[4] Hell E, Knupfer W, Mattern D. Nucl Instrum Methods Phys Res, 2000; 454A: 40[5] Duclos S J, Greskovich C D, Lyons R J, Vartuli J S, Hoffman D M, Riedner R J, Lynch M J. Nucl Instrum Methodes Phys Res, 2003; 505A: 68[6] Hong G Y, Jeon B S, Yoo Y K, Yoo J S. J Electrochem Soc, 2001; 148(11): 161[7] Yoo J S, Lee J D. J Appl Phys, 1997; 81: 2810[8] Schaik W V, Blasse G. Chem Mater, 1992; 4: 410[9] Mishra K C, Berkowitz J K, Johnson K H, Schmidt P C. Phys Rev, 1992; 45B: 10902[10] Ji Y M, Jiang D Y, Qin L S, Chen J J, Feng T, Liao Y K, Xu Y P, Shi J L. J Cryst Growth, 2005; 280: 93[11] Villanueva–Iba˜nez M, Le Luyer C, Parola S, Dujardin C, Mugnier J. Opt Mater, 2005; 27: 1541[12] Ji Y M, Jiang D Y, Wu Z H, Feng T, Shi J L. Mater Res Bull, 2005; 40: 1521[13] R´etot H, Bessi`ere A, Kahn–Harari A, Viana B. Opt Mater, 2008; 30: 1109[14] Dole S L, Venkataramani S. US Pat 5124072, 1992[15] Kintaka Y J, Kuretake S, Tanaka N, Kageyama K, Takagi H. J Am Ceram Soc, 2010; 93: 1114[16] Moon C, Nishi M, Miura K, Hirao K. J Lumin, 2009; 129: 817[17] Liu X H, Wang X D. Opt Mater, 2007; 30: 626[18] Haberko K, Ciesla A, Pron A. Ceramurgia Int, 1975; 1(3): 111[19] Zhang J C, Wen Z Y, Huang S H, Wu J G, Han J D. Ceram Int, 2008; 34: 1273[20] Pan J H, Zhang X W, Du A J H, Sun D D, Leckie J O. J Am Chem Soc, 2008; 130: 11256 |
|