| 铁-钛-碳及铁-硅-钛-碳熔体中钛与碳的溶解度 |
| 彭瑞伍;邹元爔 |
| 中国科学院冶金研究所;中国科学院冶金研究所 |
|
| THE SOLUBILITY OF Ti AND C IN Fe-Ti-C AND Fe-Si-Ti-C MELTS |
| PENG HSUI-WU;CHOU YUAN-HSI Institute of Metallurgy;Academia Sinica |
引用本文:
彭瑞伍;邹元爔. 铁-钛-碳及铁-硅-钛-碳熔体中钛与碳的溶解度[J]. 金属学报, 1963, 6(2): 111-120.
,
.
THE SOLUBILITY OF Ti AND C IN Fe-Ti-C AND Fe-Si-Ti-C MELTS[J]. Acta Metall Sin, 1963, 6(2): 111-120.
[1] 彭瑞伍、邹元燨:科学通报,1958,16,449. [2] #12 [3] Delve,F.D.,Mayer,H.W.:Met.Soc.Conf.,1961,8,1111-1137. Delve,F.D.:Trans.AIME.1958,212. 183. [4] 邹元燨:金属学报,1956,1,7. [5] Chipman,J.,Robert,M.:Trans.Am.Soc.Metals,1952,44,1215. [6] 三本木贡治等:东北大学选矿制炼研究所汇报,1956,12,(2) ,99. [7] Richardson,F.D.:J.Iron Steel Inst.,1953,175,33. [8] Chipman,J.:Basic Open Hearth Steelmaking,2nd ed.,(AIME,1951) ,p.573. [9] Skinner,G.,Johnston,H.L.,Beckett,C.:Titanium and its Compounds,(Johnston,H.L.,Enterprises,Columbus,Ohio,1954) . [10] Ohtani,M.,Gokcen,N.A.:Trans.AIME,1960,218,533. [11] Rise,A.,Chipman,J.:Physical Chemistry of Steelmaking,(Wiley,1958) ,p.3. [12] Chipman,J.:Basic Open Hearth Steelmaking,2nd ed.,(AIME,1951) ,p.669. [13] Chipman,J.:Trans.AIME,1960,218,767. [14] Neumann,F.,Schenck,H.:Arch.Eisenhüttenwesen.,1959,30,477. [15] Fuwa,T.,Chipman,J.:Trans.AIME,1959. 215,709. [16] Richardson,F.D.,Dennis,W.E.:Trans.Faraday Soc.,1953,49,171. [17] Wagner,C.:Thermodynamics of Alloys,(Addison-Wesley Press,Inc.,1952) ,p.51. [18] Turkdogan,E.T.:J.Iron Steel Inst.,1955,179,37. [19] Comstock,G.F.,Titanium in Iron and Steel,(Wiley,1955) ,p.21. [20] 泽村 宏、盛 利贞、津田昌利:铁と铜,1957,43,561。 [21] Bishop,H.L.:Trans.AIME,1959,215,171. [22] 著,北京钢铁学院冶金系炼铁教研组译:炼铁学,(高等教育出版社,1955年),2卷,2分册,125页。 [23] #12 [24] 俵国一、长谷川熊彦:砂铁,(工业图书株式会社,1941年),213页。 [25] 谷口光平、八本贞之助:铁と钢,1949,35,2.j |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|