| 锆在钼合金中的内吸附及其对再结晶温度和高温力学性能的影响 |
| 吴平森;庄育智 |
|
| INTERNAL ADSORPTION OF ZIRCONIUM IN MOLYBDENUM ALLOYS AND ITS EFFECT ON RECRYSTALLIZATION TEMPERATURE AND HIGH TEMPERATURE STRENGTH |
| WU PING-SEN;CHUANG YU-CHIH |
引用本文:
吴平森;庄育智. 锆在钼合金中的内吸附及其对再结晶温度和高温力学性能的影响[J]. 金属学报, 1965, 8(1): 77-81.
,
.
INTERNAL ADSORPTION OF ZIRCONIUM IN MOLYBDENUM ALLOYS AND ITS EFFECT ON RECRYSTALLIZATION TEMPERATURE AND HIGH TEMPERATURE STRENGTH[J]. Acta Metall Sin, 1965, 8(1): 77-81.
[1] Jaffee, R. I.: The Metal Molybdenum, ed. J. J. Harwood, (Am. Soc. Metals, 1958) , p. 330. [2] Semchyshen, M.: The Metal Molybdenum, ed. J. J. Harwood, (Am. Soc. Metals, 1958) , p. 281. [3] #12 [4] 科垂耳,A.N.著,葛庭燧译:晶体中的位错和范性流变,(科学出版社,196J年),202页 |
|