| 难变形镍铬钴基高温合金中σ相对合金力学性能的影响 |
| 陈淦生;姚常春;仲增墉 |
| 北京钢铁研究院;北京钢铁研究院;北京钢铁研究院 |
|
| THE EFFECT OF σ-PHASE IN CERTAIN Ni-Cr-Co BASE SUPERALLOY |
| Chen Gan-sheng Yao Chang-chun Zhong Zeng-yong(Beijing Institute of Iron and Steel Research) |
引用本文:
陈淦生;姚常春;仲增墉. 难变形镍铬钴基高温合金中σ相对合金力学性能的影响[J]. 金属学报, 1978, 14(3): 284-337.
,
,
.
THE EFFECT OF σ-PHASE IN CERTAIN Ni-Cr-Co BASE SUPERALLOY[J]. Acta Metall Sin, 1978, 14(3): 284-337.
[1] Dreshfield, R. L. and Ashbrook, R. L., NASA TND-6015, (1969) . [2] Dreshfield, R. L. and Ashbrook, R. L., NASA TN D-7654, (1974) . [3] Sims, C. T., The Superalloys, ed. by C. T. Sims and W. C. Hagel, Wiley, New York, (1972) , 259. [4] Mihslidin, J. R. et al., Trans. AIME, 242 (1968) , 2399. [5] Chaudhuri, A., J. Inst. Metals, 100 (1972) , 335. [6] Woodyatt, L. R. et al., Trans. AIME, 236 (1966) , 519.N |
|