| 两种马氏体时效不锈钢的相变和力学性能 |
| 李健纯;高安娟;王占一 |
| 中南矿冶学院;中南矿冶学院;中南矿冶学院 |
|
| PHASE TRANSFORMATION AND MECHANICAL PROPERTIES OF MARAGING STAINLESS STEELS |
| Li Jianchun;Gao Anjuan;Wang Zhanyi Central South Institute of Mining and Metallurgy |
引用本文:
李健纯;高安娟;王占一. 两种马氏体时效不锈钢的相变和力学性能[J]. 金属学报, 1979, 15(4): 472-481.
,
,
.
PHASE TRANSFORMATION AND MECHANICAL PROPERTIES OF MARAGING STAINLESS STEELS[J]. Acta Metall Sin, 1979, 15(4): 472-481.
[1] 1977, № 7, 24. [2] 1973, № 2, 43. [3] Groues, M. and Rao, S., ASM Trans. Quart., 62 (1969) , 902. [4] 1976, № 10, 21. [5] Pampillo, C. A. and Paxton, H. W., Met. Trans., 3 (1972) , 2895. [6] Zerwekh, R. P. and Wayman, C. M., Acta Met., 13 (1965) , 99. [7] Jana, S. and Wayman, C. M., Trans. AIME, 239 (1967) , 1187. [8] 1977, № 7, 31.g |
|