| 恒导磁合金磁导率稳恒性的计算 |
| 杨膺善;张安宁 |
| 冶金工业部钢铁研究总院;冶金工业部钢铁研究总院 |
|
| CALCULATION ON THE STABILITY OF THE CONSTANT PERMEABILITY ALLOY |
| Yang Yingshan;Zhang Anning Central Iron and Steel Research Institute; Ministry of Metallurgical Industry |
引用本文:
杨膺善;张安宁. 恒导磁合金磁导率稳恒性的计算[J]. 金属学报, 1979, 15(4): 489-497.
,
.
CALCULATION ON THE STABILITY OF THE CONSTANT PERMEABILITY ALLOY[J]. Acta Metall Sin, 1979, 15(4): 489-497.
[1] Bozorth, R. M., Ferromagnetism, D. Van Nostrand, London, 1951. p. 579. [2] 杨膺病善,王振昌,王崇愚,陈新华,金属学报11(1975) ,196. [3] Taniguchi, S., Sci. Rep. Res. Inst. Tohoku Univ., Ser. A, 8 (1956) , № 3, p. 173. |
|