| 淬火温度对中碳钢的组织和强韧性的影响 |
| 楼秉哲;陈希成 |
| 陕西机械学院;中国科学院物理研究所 |
|
| EFFECT OF AUSTENITIZING TEMPERATURE ON THE MICROSTRUCTURE AND FRACTURE TOUGHNESS OF A MEDIUM CARBON CrMnMo STEEL |
| Lou Bingzhe;Chen Xicheng Shaanxi Mechanical Engineering Institute Institute of Physics; Academia Sinica |
引用本文:
楼秉哲;陈希成. 淬火温度对中碳钢的组织和强韧性的影响[J]. 金属学报, 1979, 15(4): 498-589.
,
.
EFFECT OF AUSTENITIZING TEMPERATURE ON THE MICROSTRUCTURE AND FRACTURE TOUGHNESS OF A MEDIUM CARBON CrMnMo STEEL[J]. Acta Metall Sin, 1979, 15(4): 498-589.
[1] Lai, G. Y., Wood, W. E., Clark, R. A., Zackay, V. F. and Parker, E. R., Met. Trans., 5 (1974) , 1663. [2] Zackay, V. F., Parker, E. R. and Wood, W. E., Microstructure and Design of Alloys, International Conference on the Strength of. Metals and Alloys, 3d, Cambridge, Eng., 1973, Vol. 1, p. 175. [3] Beachem, C. D., Met. Trans., 4 (1973) , 1999. [4] Thomas, G., Iron and Steel Inter., 46. (1973) , 451. [5] Das, S. K. and Thomas, G., ASM Trans. Quart., 62 (1969) , 659. [6] Hahn, G. T. and Rosenfield, A. R., Applications Related Phenomena in Titanium Alloys, Amer. Soc. Test. Mater., Spec. Tech. Publ. №. 432, 1968, p. 5 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|