| Ti-679合金在高温空气中氧的玷污 |
| 万晓景;曹名洲;辛公春 |
| 中国科学院金属研究所;中国科学院金属研究所;黎明机械厂 |
|
| OXYGEN CONTAMINATION OF Ti-679 ALLOY UNDER HIGH TEMPERATURE |
| Wan Xiaojing;Cao Mingzhou;Xin Gongchun Institute of Metal Research; Academia Sinica Liming Machine Works |
引用本文:
万晓景;曹名洲;辛公春. Ti-679合金在高温空气中氧的玷污[J]. 金属学报, 1979, 15(4): 563-565.
,
,
.
OXYGEN CONTAMINATION OF Ti-679 ALLOY UNDER HIGH TEMPERATURE[J]. Acta Metall Sin, 1979, 15(4): 563-565.
|