金属学报  1981, Vol. 17 Issue (3): 253-258    
  论文 本期目录 | 过刊浏览 |
金属材料力学性能与斜裂纹断裂临界角的关系
龙期威
中国科学院金属研究所
RELATIONSHIP BETWEEN MECHANICAL PROPERTY OF METALS AND CRITICAL FRACTURE ANGLE OF A SLANTED CRACK
by Long Qiwei (Lung Chi-wei) (Institute of Metal Research; Academia Sinica)
引用本文:

龙期威. 金属材料力学性能与斜裂纹断裂临界角的关系[J]. 金属学报, 1981, 17(3): 253-258.
. RELATIONSHIP BETWEEN MECHANICAL PROPERTY OF METALS AND CRITICAL FRACTURE ANGLE OF A SLANTED CRACK[J]. Acta Metall Sin, 1981, 17(3): 253-258.

全文: PDF(470 KB)  
摘要: 本文提出并应用两个临界角的概念对斜裂纹断裂问题,特别是有关试验的选材问题进行了讨论;并指出,迄今为止国内外试验用过的金属材料作为判断小角度的斜裂纹拉伸问题都是不够理想的。
Abstract:New concept of two critical angles was suggested to fracture analysis of a slanted crack. A discussion was especially made of the material choice for small slant angle experiment. It is shown that all the metallic materials which used to be conventionally employed in such experiments seem to be not most satisfactory.
收稿日期: 1981-03-18     
[1] 1976年北京断裂力学交流会第二次会议文集,1977,p.302,340.
[2] Hussain, M. A. Pu, S. L. and Underwood, J., Amer. Soc. Test. Mater., Spec. Tech. publ., № 560, 1973, p. 2.
[3] Hellen, T. K. and Blackburn, W. S., Int. J. Fracture, 11 (1975) , 605.
[4] 王仁东,1976年北京断裂力学交流会第二次会议论文集,1977,p.340.
[5] 高桦、王自强、杨成寿、周爱华,金属学报,15(1979) ,380.
[6] 龙期威,金属学报,12(1976) ,63.
[7] Lung Chi-Wei (龙期威), Preprint of the International Centre for Theoretical Physics, IC/79/72, 1979, Trieste Italy; Sci. Sinica, 23 (1980) , 441.
[8] Sih, G. C. and Macdonald, B., Eng. Fract. Mech., 6 (1974) , 361.
[9] Williams, J. G. and Ewing, P. D., Int. J. Fract. Mech. 8 (1972) , 441.
[10] Shah, R. C., Amer. Soc. Test. Mater., Spec. Tech. Publ., № 560, 1973, p. 29.
[11] 金属研究所,冶金系统第一届断裂韧性工作经验交流会资料选编,冶金部情报标准研究所,1976,p.132.
[12] 东北工学院,铸铁及其熔化,冶金工业出版社,1978,p.49.
[13] Marshall, G. P., Coutts, L. H. and Williams, J. G., J. Mat. Sci., 9 (1974) , 1409.
[14] Damage Tolerant Desigh Handbook, (MCIC-HB-01) , Columbus, Ohio. 1973.
[15] Knott, J. F., Fuodamentals of Fracture Mechanics, Butterworths, London, 1973, p. 112.
No related articles found!