| 冷拉Si-Cr气阀钢的断裂力学分析 |
| 殷匠;许经峰 |
| 上海第五钢铁厂;上海第五钢铁厂 |
|
| FRACTURE-MECHANICS ANALYSIS OF COLD-DRAWN Si-Cr VALVE STEEL |
| by Yin Jiang and Xu Jingfeng (Shanghai No. 5 Steel Works) |
引用本文:
殷匠;许经峰. 冷拉Si-Cr气阀钢的断裂力学分析[J]. 金属学报, 1981, 17(3): 259-365.
,
.
FRACTURE-MECHANICS ANALYSIS OF COLD-DRAWN Si-Cr VALVE STEEL[J]. Acta Metall Sin, 1981, 17(3): 259-365.
[1] #12 [2] #12 [3] #12 [4] 钢铁研究院断裂韧性研究组,金属学报,13(1978) ,214. [5] 小坂田宏造,塑性加工,9(1978) ,665. [6] Elber, W., Fracture Toughness and Slow-Stable Cracking, Proc. 1973 National Symp. Fract. Mech., Part 1, ed. by P. C. Paris, (ASTM STP 559) , ASTM, 1974, p. 45. [7] Sin, G. C., Handbook of Stress-Intensity Factors, Inst. of Fracture and Solid Mech., Bethlehem, Pennsylvania, 1973, p. 1. 3. 1-1; [8] Rooke, D. P. and Cartwight, D. J., Compendium of Stress Intensity Factors, HMSO, London, 1976, p. 233. [9] 未发表工作. |
|