| 金属玻璃Fe_(78)Si_(10)B_(12)的感生磁各向异性 |
| 陈笃行 |
| 冶金工业部钢铁研究总院 |
|
| ON THE INDUCED MAGNETIC ANISOTROPY OF METALLIC GLASS Fe__(78)Si_(10)B_(12) |
| CHEN Duxing (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 24 May; 1983; revised manuscript 17 November; 1983) |
引用本文:
陈笃行. 金属玻璃Fe_(78)Si_(10)B_(12)的感生磁各向异性[J]. 金属学报, 1984, 20(5): 441-445.
.
ON THE INDUCED MAGNETIC ANISOTROPY OF METALLIC GLASS Fe__(78)Si_(10)B_(12)[J]. Acta Metall Sin, 1984, 20(5): 441-445.
1 陈笃行,金属学报,20(1984) .B212. 2 Gibbs, M. R. J. ; Evetts, J. E. ; Leake, J. A. , Activation Energy Spectra and Relaxation in Amorphous Materials, 1982, (preprint). 3 Egami, T. ; Flanders P. J. , AIP Conf. Proc. , 29 (1976) , 220. 4 Allia, P. ; Soardo, G. P. ; Vinai, F. , Solid State Commun. , 24 (1977) , 517. 5 O'Handley, R. C. , Phys. Rev. , B18 (1978) , 930. 6 Luborsky, F. E. , AIP Conf. Proc. , 29 (1976) , 209. 7 Egami, T. , Amorphous Metallic Alloys, Ed. Luborsky, F. E. , Butterworths, London, 1983 (Preprint). |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|