    					| LiF-KCl系和LiF-KBr系的熔盐电导 | 
  					 
  					  										
						| 徐驰;刘国梁;陈念贻 | 
					 
															
					| 中国科学院上海冶金研究所;中国科学院上海冶金研究所;中国科学院上海冶金研究所 | 
					 
										
						 | 
					 
   										
    					| SPECIFIC CONDUCTANCE OF MOLTEN LiF-KCl OR LiF-KBr SYSTEM | 
  					 
  					  					  					
						| XU Chi; LIU Guoliang; CHEN Nianyi (Shanghai Institute of Metallurgy; Academia Sinica) (Manuscript received 10 January; 1983) | 
					 
														 
				
				引用本文: 
				
								徐驰;刘国梁;陈念贻. LiF-KCl系和LiF-KBr系的熔盐电导[J]. 金属学报, 1984, 20(5): 446-448.	
																												 																				 ,
																								 ,
																												 . 
				SPECIFIC CONDUCTANCE OF MOLTEN LiF-KCl OR LiF-KBr SYSTEM[J]. Acta Metall Sin, 1984, 20(5): 446-448.	                                                        				  
				
				
					
						
							
								
									
									
									
									
									 
          
          
            
                         
            
									            
									                
																														  