    					| 金属玻璃Fe_(78)Si_(10)B_(12)的感生磁各向异性 | 
  					 
  					  										
						| 陈笃行 | 
					 
															
					| 冶金工业部钢铁研究总院 | 
					 
										
						 | 
					 
   										
    					| ON THE INDUCED MAGNETIC ANISOTROPY OF METALLIC GLASS Fe__(78)Si_(10)B_(12) | 
  					 
  					  					  					
						| CHEN Duxing (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) (Manuscript received 24 May; 1983; revised manuscript 17 November; 1983) | 
					 
														 
				
				引用本文: 
				
								陈笃行. 金属玻璃Fe_(78)Si_(10)B_(12)的感生磁各向异性[J]. 金属学报, 1984, 20(5): 441-445.	
																												 																								 . 
				ON THE INDUCED MAGNETIC ANISOTROPY OF METALLIC GLASS Fe__(78)Si_(10)B_(12)[J]. Acta Metall Sin, 1984, 20(5): 441-445.	                                                        				  
				
				
					
						
							
								
									
									
									
									
									 
          
          
            
                         
            
									            
									                
																														  
																  1 陈笃行,金属学报,20(1984) .B212.  2 Gibbs, M. R. J. ; Evetts, J. E. ; Leake, J. A. , Activation Energy Spectra and Relaxation in Amorphous Materials, 1982, (preprint). 3 Egami, T. ; Flanders P. J. , AIP Conf. Proc. , 29 (1976) , 220.  4 Allia, P. ; Soardo, G. P. ; Vinai, F. , Solid State Commun. , 24 (1977) , 517.  5 O'Handley, R. C. , Phys. Rev. , B18 (1978) , 930.  6 Luborsky, F. E. , AIP Conf. Proc. , 29 (1976) , 209.  7 Egami, T. , Amorphous Metallic Alloys, Ed. Luborsky, F. E. , Butterworths, London, 1983 (Preprint). | 
															   
																													 
									             
									           
             
			            			 
			 
             
												
											    	
											        	 | 
											        	Viewed | 
											         
													
											        	 | 
											        	 | 
											         
											      	
												         | 
												        
												        	Full text 
												          	
												         | 
											        	
												        	
												        	 
												        	
												          	 
												          	
												          	
														 | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        
												        	Abstract 
												          	
														 | 
												        
															
															 
															
															
												         | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        Cited  | 
												        
												        	
												         | 
													 
													
												         | 
												         | 
												         | 
													 
													
													    |   | 
													    Shared | 
													       | 
												  	 
												  	
													     | 
													     | 
													     | 
											  		 
											  		
													    |   | 
													    Discussed | 
													       | 
												  	 
											 
											 
             
           
      
									
									
		
									
									
									
									
									
									 | 
								 
							 
						 | 
					 
				 
			
		 |