| 非晶(Fe_(0.1)Ni_(0.35)Co_(0.55))_(78)Si_8B_(14)和Fe_(40)Ni_(38)Mo_4B_(18)合金的磁导率弛豫 |
| 张延忠;程东;张东平 |
| 上海钢铁研究所;上海钢铁研究所;上海钢铁研究所 |
|
| MAGNETIC PERMEABILITY RELAXATIONS IN AMORPHOUS ALLOYS(Fe_(0.1)Ni_(0.55)Co_(0.55))_(78)Si_8B_(14) AND Fe_(40)Ni_(38)Mo_4B_(18) |
| ZHANG Yanzhong;CHENG Dong;ZHANG Dongping Shanghai Iron and Steel Research Institute |
引用本文:
张延忠;程东;张东平. 非晶(Fe_(0.1)Ni_(0.35)Co_(0.55))_(78)Si_8B_(14)和Fe_(40)Ni_(38)Mo_4B_(18)合金的磁导率弛豫[J]. 金属学报, 1985, 21(3): 99-105.
,
,
.
MAGNETIC PERMEABILITY RELAXATIONS IN AMORPHOUS ALLOYS(Fe_(0.1)Ni_(0.55)Co_(0.55))_(78)Si_8B_(14) AND Fe_(40)Ni_(38)Mo_4B_(18)[J]. Acta Metall Sin, 1985, 21(3): 99-105.
1 张延忠;金慧娟,金属学报,20(1984) ,B78. 2 Matsuyama,T.;Ohta,K.;Kajiura,M.;Teranishi,T.,Jpn.J.Appl.Phys.,19(1980) ,55. 3 Nose,M.;Esashi,K.;Kanehira,J.;Ohnuma,S.;Shirakawa,K.;Masumoto,T.,Proc.4th Int.Conf.on Rapidly Quenched Metals,Vol.1,Eds.Masumoto,T.;Suzuki,K.(?)IM,1982,p.1191. 4 Mizoguchi,T.;Hatta,S.;Akiyama,K.;Maeda,K.;Takayama,S.,ibid.,p.1195. 5 Egami,T.,J.Magn.Magn.Mater.,31-34(1983) ,1571. 6 Phillips,D.L.,J.Assoc.Comput.Mach.,9(1962) ,84. 7 Hesse,J.;Rübartsch,A.,J.Phys.,E7(1974) ,526. 8 Kronmüller,H.,Philos.Mag.,B48(1983) ,127. 9 Kronmüller,H.,J.Magn.Magn.Mater.,41(1984) ,366. 10 Egami,T.;Maeda,K.;Vitek,V.,Philos.Mag.,A41(1980) ,883. 11 Srolovitz,D.;Maeda,K,;Vitek,V.;Egami,T.,Philos.Mag.,A44(1981) ,847. 12 Egami,T.;Srolovitz,D.,J.Phys.,F12(1982) ,2141. 13 Allia,P.;Soardo,G.P.;Vinai,F.,J.Magn.Magn.Mater.,31-34(1983) ,1527. 14 Allia,P.;Vinai,F.,Phys.Rev.,B26(1982) ,6141. 15 Allia,P.;Beatrice,C.;Schneider,J.,J.Magn.Magn.Mater.,42(1984) ,148. 16 Allia,P.;Sato Turtelli,R.;Vinai,F.;Riontino,G.,Solid State Commun.,43(1982) ,821. 17 张延忠,金属学报,20(1984) ,B195. 18 Chambron,W.;Chamberod,A.,Solid State Commun.,35(1980) ,61 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|