| 非晶态合金Ni-P和Pd-Ni-P的电子结构 |
| 冯平义;陈念贻;俞志中;廖沐真;郭金梁 |
| 中国科学院上海冶金研究所;中国科学院上海冶金研究所;上海市测试技术研究所;清华大学;清华大学 |
|
| THE ELECTRONIC STRUCTURE OF AMORPHOUS ALLOYS Ni-P AND Pd-Ni-P |
| FENG Pingyi;CHEN Nianyi Shanghai Institute of Metallurgy;Academia Sinica;YU Zhizhong Shanghai Institute of Testing Technics;LIAO Muzhen;GUO Jinliang Tsinghua University;Beijing |
引用本文:
冯平义;陈念贻;俞志中;廖沐真;郭金梁. 非晶态合金Ni-P和Pd-Ni-P的电子结构[J]. 金属学报, 1985, 21(3): 106-114.
,
,
,
,
.
THE ELECTRONIC STRUCTURE OF AMORPHOUS ALLOYS Ni-P AND Pd-Ni-P[J]. Acta Metall Sin, 1985, 21(3): 106-114.
1 Polk,D.E.,Scr.Metall.,4(1970) ,117. 2 Hasegawa,R,;Hines,W.A.;Kabacoff,L.E.;Duwez,P.,Solid State Commun.,20(1976) ,1035. 3 O' Handley,R.C.;Boudreaux,D.S.,Phys.Status Solidi,(a)45(1978) ,607. 4 Hines,W.A.;Kabacoff,L.T.;Hasegawa,R.;Duwez,P.,J.Appl.Phys.,49(1978) ,1724. 5 Fuggle,J.C.,Phys.Rev.,B 27(1983) ,2145. 6 Amamou,A.;Krill,G.,Solid State Commun.,33(1980) ,1087. 7 Bakonyi,I.;Kovacs,I.;Varga,L.;Bagi.T.;Lovas,A.;Tothkader,E.;Tompa,K.,Proc.of the Conf.on Metallic Glasses Science and Technology(Budapest,1980) . 8 Hines.W.A.,Solid State Commun.,39(1981) ,699. 9 Binder,H.;Fluck,E.,Modern Physics in Chemistry,Vol.2,Eds.Fluck,E.;Goldanskii,V.I.,Academic Press,London,1979,p.321. 10 Messmer,R.P.,Phys.Rev.,B 23(1981) ,1616. 11 Hasegawa,R.;O' Handley,R.C.;Mendelson,L.I.,Magnetism and Magnetic Materials,AIP.Conf.Proc.№34,AIP.Publ.,New York,1976,p.298. 12 Hines.W.A.;Lawrence,T.;Kabacoff,L.E.;Hasegawa,R.;Duwez,P.,Amorphous Magnetism,II,Eds.Levy,R.A.;Hasegawa,R.,Plenum Press,New York,1977,p.207. 13 Hines,W.A.;Modzelewski,C.U.;Paolino,R.N.;Chen,H.S.,J.Appl.Phys.,52(1981) ,1814. 14 Hines,W.A.;Clover,K.;Clark,W.G.;Kabacoff,L.T.;Modzelewski,C.U.;Hasegawa,R.;Duwez,P.,Phys.Rev.,B 21(1980) ,3771. |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|