| 第二类超导体在低温下的磁性 |
| 戴问民 |
| 北京钢铁学院 |
|
| MAGNETIC PROPERTIES OF TYPE II SUPERCONDUCTORS AT LOW TEMPERATURE |
| DAI Wenmin Beijing University of Iron and Steel Technology |
引用本文:
戴问民. 第二类超导体在低温下的磁性[J]. 金属学报, 1985, 21(4): 45-56.
.
MAGNETIC PROPERTIES OF TYPE II SUPERCONDUCTORS AT LOW TEMPERATURE[J]. Acta Metall Sin, 1985, 21(4): 45-56.
1 #12 2 #12 3 #12 4 Werthamer,N.R.,Phys.Rev.,123(1963) ,663. 5 王竹溪,未发表资料,1973. 6 Caroli,C.,Phys.Lett.,9(1964) ,307. 7 Maki,K.;Tsuzuki,T.,Phys.Rev.,139(1965) ,A868 McConville,T.;Serin,B.,Phys.Rev.,140(1965) ,A1169. |
|