| 球化碳钢中的碳化物开裂 |
| 张以增;刘湘杰 |
| 华中工学院;华中工学院;长沙矿冶研究院 |
|
| CARBIDE PARTICLE CRACKING IN SPHEROIDIZED CARBON STEELS |
| ZHANG Yizeng;LIU Xiangjie Huazhong University of Science and Technology;Wuhan |
引用本文:
张以增;刘湘杰. 球化碳钢中的碳化物开裂[J]. 金属学报, 1985, 21(4): 57-62.
,
.
CARBIDE PARTICLE CRACKING IN SPHEROIDIZED CARBON STEELS[J]. Acta Metall Sin, 1985, 21(4): 57-62.
1 Argon,A.S.;Im,J.;Safoglu,R.,Metall.Trans.,6A(1975) ,839. 2 Fisher,J.R.;Guriland,J.,Met.Sci.,15(1981) ,193. 3 Lc Roy,G.;Embury,J.D.;Edward,G.;Ashby,M.F.,Acta Metall.,29(1981) ,1509. 4 张以增,金属学报,19(1983) ,A70. 5 Zou,H.-C.;Lou,Y.-L.;Zhang,Y.-Z.,Met.Sci Eng.,62(1984) ,163. 6 Gurland,J.,Acta Metall.,20(1972) ,735. 7 Inoue,T.;Kinoshita,S.,The Microstructure and Design of Alloys,Proc.of the 3rd Int.Conf.on the Strength of Metals and Alloys,Cambridge,England,Aug.20,1973,Sponsored by The Inst.of Metals and The Iron and Steel Inst.,Vol.1,paper 32,1973,p.159. 8 Needleman,A.,J.Mech.Phys.Solids,20(1970) ,111. 9 McCormick,C.W.,NASTRAN Users Manual,Level 15. 5,Document NASA ST[(222) 01] ,NASA,Washington,DC.,1973. 10 Kelly,A.,Strong Solids,Oxford Univ.Press,1966,p.9 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|