| Ce对Fe-Cr合金氧化膜织构的作用 |
| 高怀荪;李碚 |
| 包头冶金研究所;包头冶金研究所 |
|
| EFFECT OF Ce ON PREFERRED ORIENTATION OF GRAIN IN OXIDE SCALE ON Fe-15Cr ALLOY |
| by GAO Huaisun;LI Bei Baotou Research Institute of Metallurgy |
引用本文:
高怀荪;李碚. Ce对Fe-Cr合金氧化膜织构的作用[J]. 金属学报, 1985, 21(6): 44-49.
,
.
EFFECT OF Ce ON PREFERRED ORIENTATION OF GRAIN IN OXIDE SCALE ON Fe-15Cr ALLOY[J]. Acta Metall Sin, 1985, 21(6): 44-49.
1 Wood, G. C.; Boustead, J., Corros. Sci., 8 (1968) , 719. 2 Nagai H.; Okabayashi, M.; Mitani, H., Trans. Jpn Inst Met., 21 (1980) , 341. 3 天野忠昭;矢岛圣使;木村孝;齐藤安俊,防食技术,24(1975) ,19. 4 Stringer, J., Oxid. Met.,5(1972) ,11. 5 李陪;颜玉新;高怀荪;中国腐蚀防护学报,5(1985) ,(待发表). 6 Mueller, M. H.; Chernock, W. P.; Beck, P. A., Trans. Metall. Soc. AIME., 212 (1958) , 39. 7 Klug, H. D.; Alexander, L. E., X-Ray Diffraction Procedure for Poly Crystalline and Amorphous, 2nd ed., Wiley, New York, 1974,p. 360. 8 张立新;骆继勋;银耀德;李黎光;赵齐;张家芸,金属学报,17(1981) ,233. |
|