| 氢对钛合金中位错速度应力指数的影响 |
| 曹名洲;杨柯;万晓景 |
| 中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所 |
|
| EFFECT OF HYDROGEN ON DISLOCATION VELOCITY-STRESS EXPONENTS OF Ti ALLOYS |
| CAO Mingzhou YANG Ke WAN Xiaojing (Institute of Metal Research;Academia Sinica;Shenyang) |
引用本文:
曹名洲;杨柯;万晓景. 氢对钛合金中位错速度应力指数的影响[J]. 金属学报, 1987, 23(1): 92-94.
,
,
.
EFFECT OF HYDROGEN ON DISLOCATION VELOCITY-STRESS EXPONENTS OF Ti ALLOYS[J]. Acta Metall Sin, 1987, 23(1): 92-94.
1 Johnston W J,Gilman J J.J Appl Phys.1959;30:129 2 Li J C M.Can J Phys.1967;45;493 3 尹万全,苏会和,徐永波,秦荣士,刘民治.金属学报,1985;21:A323 4 Troiano A R.Trans ASM,1960;52:54 5 万暁景,杨柯,曹名洲.金属学报,1986;22:189 6 Tien J K.Metall Trans,1976;7A:821h |
|