| 关于Fe-Pb相图的几个问题 |
| 邢中枢 |
| 中国科学院金属研究所 |
|
| NOTE ON THE Fe-Pb PHASE DIAGRAM |
| XING Zhong shu (Institute of Metal Research.Academia Sinica;Shenyang) |
引用本文:
邢中枢. 关于Fe-Pb相图的几个问题[J]. 金属学报, 1987, 23(1): 115-119.
.
NOTE ON THE Fe-Pb PHASE DIAGRAM[J]. Acta Metall Sin, 1987, 23(1): 115-119.
1 Kubaschewski O,Iron-Binary Phase Diagrams,Springer-Verla.1982;87-88 2 Stevenson D A,Wulff J.Trans Metal1 Soc AIME,1961;221:271 3 Miller K O,Elliott J F,Trans Metal1 Soc AIME 1960;218:900 4 Morozov A N,Ageyev Yu A.Russ Metall,1971;4:78 5 Lord A E,Parlee N A.Trans Metall Soc AIME,1960;218:644 6 Araki T,Trans Natl Res Inst Met(Tokyo),1963;5:91 7 荒木透,小柳明,大场健二,大桥久道.铁と钢,1963;49:421 8 Kubaschewski O,High Temp High Pressures,1981;13:435 9 Kubaschewski O,Alcock C B.Metallurgical Thermochemistry,5th ed,Pergamon Press.1979 |
|