金属学报  1987, Vol. 23 Issue (1): 115-119    
  论文 本期目录 | 过刊浏览 |
关于Fe-Pb相图的几个问题
邢中枢
中国科学院金属研究所
NOTE ON THE Fe-Pb PHASE DIAGRAM
XING Zhong shu (Institute of Metal Research.Academia Sinica;Shenyang)
引用本文:

邢中枢. 关于Fe-Pb相图的几个问题[J]. 金属学报, 1987, 23(1): 115-119.
. NOTE ON THE Fe-Pb PHASE DIAGRAM[J]. Acta Metall Sin, 1987, 23(1): 115-119.

全文: PDF(374 KB)  
摘要: 对 Pb 在 Fe 液中溶解度的实验数据进行评述,从而选出合理的数值,再通过简单的热力学处理,求出其与温度的依赖关系.将此关系与凝固点下降公式结合,算出 Fe-Pb 相图中偏晶点的成分和温度.对 Fe 在 Pb 液中溶解度的实验结果也作了适当的处理.在上述工作的基础上,给出了一个 Fe-Pb 相图.
Abstract:To elucidate the relation between optimum solubility and temperature,the critical assessment of the experimental data of solubility of Pb in liquid Fe,or of Fe in liquid Pb,have been made.By combining these relations with the liquids curve calculated from Clausius-Clapeyron equation,the composition and temperature of the monotectic point on the Fe-Pb phase diagram have been esti- mated.Thus,an Fe-Pb phase diagram may be drawn on the basis of above men- tioned studies.
收稿日期: 1987-01-18     
1 Kubaschewski O,Iron-Binary Phase Diagrams,Springer-Verla.1982;87-88
2 Stevenson D A,Wulff J.Trans Metal1 Soc AIME,1961;221:271
3 Miller K O,Elliott J F,Trans Metal1 Soc AIME 1960;218:900
4 Morozov A N,Ageyev Yu A.Russ Metall,1971;4:78
5 Lord A E,Parlee N A.Trans Metall Soc AIME,1960;218:644
6 Araki T,Trans Natl Res Inst Met(Tokyo),1963;5:91
7 荒木透,小柳明,大场健二,大桥久道.铁と钢,1963;49:421
8 Kubaschewski O,High Temp High Pressures,1981;13:435
9 Kubaschewski O,Alcock C B.Metallurgical Thermochemistry,5th ed,Pergamon Press.1979
No related articles found!