| Fe中杂质-空位复合体的研究 |
| 楼永明;顾秉林;熊家炯;高乃飞 |
| 清华大学物理系;清华大学物理系;清华大学物理系;清华大学物理系 |
|
| INVESTIGATION OF IMPURITIES-VOID COMPLEX IN Fe |
| LOU Yongming; GU Binglin; XIONG Jiajiong; GAO Naifei (Department of physics; Tsinghua University; Beijing) (Manuscript received 18 September; 1985; revised manuseript 17 May; 1986) |
引用本文:
楼永明;顾秉林;熊家炯;高乃飞. Fe中杂质-空位复合体的研究[J]. 金属学报, 1987, 23(3): 234-236.
,
,
,
.
INVESTIGATION OF IMPURITIES-VOID COMPLEX IN Fe[J]. Acta Metall Sin, 1987, 23(3): 234-236.
1 Jena P, Fradin F Y, Ellis D E. Phys Rev 1979; B20: 3543 2 Hohenberg P, Kohn W. Phys Rev, 1964; 136: B864 3 Gunnarsson O, Lundqvist B I, Wilkins J W. Phys Rev, 1974; B10: 1319 4 顾秉林,楼永明,高乃飞,熊家炯。物理学报,1986:35:17 5 Brandt W, Reinheimer J. Phys Lett, 1971; 35A: 45 |
|