| Fe-Mn-Al-Cr系亚稳奥氏体区中形变马氏体的研究 |
| 田兴;张彦生 |
| 中国科学院金属研究所;中国科学院金属研究所;大连铁道学院 |
|
| DEFORMATION MARTENSITE IN METASTABLE REGION OF Fe-Mn-Al-Cr SYSTEM |
| TIAN Xing; ZHANG Yansheng (Institute of Metal Research; Academia Sinica; Shengyang) (Manuscript received 10 June; 1985; revised manuscript 17 January; 1986) |
引用本文:
田兴;张彦生. Fe-Mn-Al-Cr系亚稳奥氏体区中形变马氏体的研究[J]. 金属学报, 1987, 23(3): 237-239.
,
.
DEFORMATION MARTENSITE IN METASTABLE REGION OF Fe-Mn-Al-Cr SYSTEM[J]. Acta Metall Sin, 1987, 23(3): 237-239.
1 Angel T. J Iron Steel Inst, 1954; 177: 165 2 Ludwigson D C, Berger J A. J Iron Steel Inst, 1965; 207: 63 3 田兴,张彦生,师昌绪.金属学报,1986;22:A 101# |
|