| 等温过程中奥氏体晶界硼偏聚的非平衡特征 |
| 贺信莱;褚幼义;唐立;周振新;柯俊 |
| 北京钢铁学院;北京钢铁学院;北京钢铁学院金属物理专业;研究生;北京钢铁学院金属物理专业;研究生;北京钢铁学院 |
|
| THE NONEQUILIBRIUM CHARACTERISTIC OF BORON SEGREGATION AT AUSTENITE GRAIN BOUNDARIES DURING ISOTHERMAL HOLDING |
| by HE Xinlai; CHU Youyi; TANG Li; ZHOU Zhenxin; KE Jun (Beijing University of Iron and Steel Technology) (Manuscript received 20 June; 1985; revised manuscript 11 January; 1986) |
引用本文:
贺信莱;褚幼义;唐立;周振新;柯俊. 等温过程中奥氏体晶界硼偏聚的非平衡特征[J]. 金属学报, 1987, 23(4): 291-298.
,
,
,
,
.
THE NONEQUILIBRIUM CHARACTERISTIC OF BORON SEGREGATION AT AUSTENITE GRAIN BOUNDARIES DURING ISOTHERMAL HOLDING[J]. Acta Metall Sin, 1987, 23(4): 291-298.
1 Aust K T, Hanneman R E, Niessen P, Westbrook J H. Acta Metall, 1968; 16: 291 2 Harries D R, Marwick A D. Philiops Trans R Soc London, 1980; A 295: 197 3 Williams T M, Stonecham A M, Harries D R. Met Sci, 1976; 10: 14 4 Faulkner R G. J Mater Sci, 1981; 16: 373 5 贺信莱,褚幼义,张秀林,佘宗森,李秋萍,尹熙光.金属学报,1977;13:235 6 贺信莱,褚幼义,柯俊.金属学报,1982;18:1 7 贺信莱,褚幼义,柯俊.金属学报.1982;18:11 8 贺信莱,褚幼义,柯俊.金属学报,1983;19:A459 9 Karlsson L, Norden H. Proc JIMIS-4 Suppl to Trans Jpn Inst Met, 1986; 27: 189 10 He X L (贺信莱), Chu Y Y (褚幼义). J Phys D: Appl Phys, 1983; 16: 1145 11 褚幼义,贺信莱,唐立,徐庭栋,柯俊.金属学报,1987;23:169 12 Veno M, Jnoue T. Trans Iron Steel Inst Jpn, 1973; 13: 210 |
|