| 位错表面像力对裂端范性区位错平衡分布的影响 |
| 刘速;熊良钺;龙期威 |
| 中国科学院金属研究所;中国科学院金属研究所;中国科学院金属研究所 |
|
| EFFECT OF DISLOCATION IMAGE FORCE ON DISLOCATION DISTRIBUTION IN PLASTIC ZONE AT CRACK TIP |
| by LIU Su; XIONG Liangyue; LONG Qiwei(C. W. Lung)(Institute of Metal Research; Academia Sinica; Shenyang)(Manuscript received 17 July; 1985; revised manuscript 17 April; 1986) |
引用本文:
刘速;熊良钺;龙期威. 位错表面像力对裂端范性区位错平衡分布的影响[J]. 金属学报, 1987, 23(5): 349-355.
,
,
.
EFFECT OF DISLOCATION IMAGE FORCE ON DISLOCATION DISTRIBUTION IN PLASTIC ZONE AT CRACK TIP[J]. Acta Metall Sin, 1987, 23(5): 349-355.
1 龙期威,熊良钺.物理学报,1984;33:755 2 Bilby B A, Cottrell A H, Swinden K H. Proc R Soc London, 1963; A272: 304 3 Kobayashi S, Ohr SM. Philos Mag, 1980; A42: 763 4 Chang SJ, Ohr SM. JAppl Phys, 1981; 52: 7174 5 Lung CW, Xiong L Y. Phys Status Solidi, (a), 1983; 77: 81 6 Jiang J, Xiong L Y, Lung C W, Ji G K, Liu N Q, Wang S Y. In: Coleman P G et al eds., Proc 6th Int Conf Positron Annihilation, held at Arlington, New York: North-Holland, 1982: 469= |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|